介绍了镁合金变形过程中孪生的晶体学、位错机理以及几何位向学;探讨了孪晶的形核、长大与演变机制;分析了孪生过程对塑性变形的作用;论述了影响孪生的几种基本因素,包括晶粒取向、变形温度、变形速度、晶粒尺寸、预变形.研究结果表明,镁合金塑性变形过程中孪生变形的作用在于,通过孪生过程改变晶粒取向或通过孪晶间或孪晶与滑移之间的相互作用,诱发新的滑移和孪生;孪晶也可抑制裂纹的产生和扩展,从而提高变形镁合金的室温塑性.

参考文献

[1] Bohlen J;Chmelik F;Dobron P et al.[J].Journal of Alloys and Compounds,2004,378:214.
[2] 陈振华,夏伟军,程永奇,傅定发.镁合金织构与各向异性[J].中国有色金属学报,2005(01):1-11.
[3] Staroselsky A.;Anand L. .A constitutive model for hcp materials deforming by slip and twinning: application to magnesium alloy AZ31B[J].International Journal of Plasticity,2003(10):1843-1864.
[4] Jager A;Lukac P et al.[J].Journal of Alloys and Compounds,2004,378:184.
[5] Christian J W;Mahajan S .[J].Progress in Materials Science,1995,39(01)
[6] Serra A;Bacon D J .[J].Philosophical Magazine,1986,54:793.
[7] Pond RC;Bacon D J;Serra A .[J].Philosophical Magazine Letters,1995,71:275.
[8] Bacon D J;Serra A.[M].Pittsburgh:TMS,1994:83.
[9] Yoo M H;Lee J K .[J].Philosophical Magazine,1991,63:987.
[10] Yoo M H;Fu C L;Lee J K .[J].Journal of Physics,1991,1:1065.
[11] Agnew S R;Horton J A;Yoo M H .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2002,33A:851.
[12] Mahajan S;Williams D F .[J].International Metals Reviews,1973,18:43.
[13] 陈振华.变形镁合金[M].北京:化学工业出版社,2005:81.
[14] 钟家湘;郑秀华;刘颖.金属学教程[M].北京:北京理工大学出版社,1995:309.
[15] Mathis K;Chmelik F;Trojanova Z et al.[J].Materials Science and Engineering A,2004,387-389:331.
[16] Mendelson S .[J].Journal of Applied Physics,1970,41:1893.
[17] Yoo M H;Loh BT M.[M].Washington:Nat Bur Stand,1970:479.
[18] Nave M D;Barnett M R .[J].Scripta Materialia,2004,51:881.
[19] 杨平,崔凤娥,边建华,G Gottstein.Relationships between deformation mechanisms and initial textures in polycrystalline magnesium alloys AZ31[J].中国有色金属学会会刊(英文版),2003(02):280-284.
[20] Yang P;Yu Y;Chen L et al.[J].Scripta Materialia,2004,50:1163.
[21] 杨平,毛卫民,任学平,唐全波.Shear bands in magnesium alloy AZ31[J].中国有色金属学会会刊(英文版),2004(05):851-857.
[22] Koike J;Kobayashi T;Mukai T et al.[J].Acta Materialia,2003,51:2055.
[23] Yoo M H;Morris J R;Ho K M et al.[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2002,33:813.
[24] Yoo M H;Agnew S R;Morris J R et al.[J].Materials Science and Engineering A,2001,319-321:87.
[25] Yoo M H .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1981,12:409.
[26] Serra A;Bacon D J .[J].Philosophical Magazine,1996,73:333.
[27] Serra A;Bacon D J .[J].Metallic Functional Materials(in Chinese)(金属功能材料),1995,43:4465.
[28] Serra A;Bacon D J.[J].Acta Metallurgica Sinica,1988(12):3273.
[29] Yoo M H .[J].Transactions of the Metallurgical Society of AIME,1969,245:2051.
[30] Yin DL;Zhang KF;Wang GF;Han WB .Warm deformation behavior of hot-rolled AZ31 Mg alloy[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2005(1/2):320-325.
[31] Myshlyaev MM.;McQueen HJ.;Mwembela A.;Konopleva E. .Twinning, dynamic recovery and recrystallization in hot worked Mg-Al-Zn alloy[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2002(1/2):121-133.
[32] Sitdikov O;Kaibyshev R;Sakai T .[J].Materials Science Forum,2003,419-422:521.
[33] 郭强,严红革,陈振华,张辉.AZ31镁合金高温热压缩变形特性[J].中国有色金属学报,2005(06):900-906.
[34] Galiyev A;Kaibyshev R;Gottstein G .[J].Acta Materiae Compositae Sinica,2001,49:1199.
[35] Serra A;Bacon D J;Pond R C .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2002,33:809.
[36] Serra A;Bacon D J .[J].Philosophical Magazine A:Physics of Condensed Matter:Structure,Defects and Mechanical Properties,1991,61:1001.
[37] Seera A;Pond R C et al.[J].Metallic Functional Materials(in Chinese)(金属功能材料),1991,39:1469.
[38] Morozumi S;Kikuchi M et al.[J].Transactions of the Japan Institute of Materials,1976,17:158.
[39] Minonishi Y;Morozumi S;Yoshinaga H .[J].Scripta Metallurgica et Materialia,1982,16:427.
[40] Minonishi Y;Morozumi S;Yoshinaga H .[J].Scripta Metallurgica et Materialia,1985,19:1241.
[41] Minonishi Y;Yoo M H .[J].Philosophical Magazine Letters,1990,61:203.
[42] Womsiewicz B C;Backofen W A .[J].Transactions AIME,1967,239:1422.
[43] Bohlen J et al.[J].Journal of Alloys and Compounds,2004,378:207.
[44] 吕宜振 .Mg-Al-Zn合金组织、性能、变形和断裂行为研究[D].上海交通大学,2001.
[45] Barnett M R .[J].Journal of Light Metals,2001,1:167.
[46] Mathis K;Trojanova Z;Lukac P et al.[J].Journal of Alloys and Compounds,2004,378:176.
[47] Klimanel P;Potzsch A .[J].Materials Science and Engineering A,2002,324:145.
[48] Perex-Prado M T;Valle J A;Ruano O A .[J].Scripta Materialia,2004,50:667.
[49] Caceres C H;Sumitomo T;Veidt M .[J].Acta Materialia,2003,51:6211.
[50] Barnett M R;Keshavara Z;Beer A G et al.[J].Acta Materialia,2004,52:5093.
[51] Kleiner S;Uggowitzer P J .[J].Materials Science and Engineering A,2004,379:258.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%