以3,5-二硝基溴苯与对甲基苯酚为原料,合成出中间产物3,5-二硝基-4'-甲基-二苯基醚,再用钯/碳还原得到芳香二胺单体3,5-二氨基-4'-甲基-二苯基醚,以此芳香二胺和四种不同芳香二酐为单体,通过低温聚合反应合成了高分子量的聚酰胺酸,热亚胺化的产物在极性强的溶剂中具有较好的溶解性.差示扫描量热(DSC)和热重法(TG)测试表明其玻璃化转变温度(Tg)介于200℃~211℃,在氮气气氛中5%,10%的热失重温度(Td)分别在520℃,535℃以上.力学性能测试表明这些可溶性聚酰亚胺薄膜的拉伸强度,弹性模量分别能达到154.19 MPa,2.85 GPa.
参考文献
[1] | Shang ZP;Lu CL;Zhao JY;Yan JL;Ding MX;Gao LX .One-pot synthesis of polyetherimides from bis(chlorophthalimide) and dichlorodiphenylsulfone in diphenylsulfone[J].Journal of Applied Polymer Science,2006(5):4584-4588. |
[2] | Zhiming Qiu;Suobo Zhang .Synthesis and properties of organosoluble polyimides based on 2,2'-diphenoxy-4,4',5,5'-biphenyltetracarboxylic dianhydride[J].Polymer: The International Journal for the Science and Technology of Polymers,2005(5):1693-1700. |
[3] | Yang CP.;Chen RS.;Wei CS. .New soluble poly(amide-imide-imide)s based on tetraimide-dicarboxylic acid condensed from 4,4 '-oxydiphthalic anhydride, 2,2-bis[4-(4-aminophenoxy)phenyl]sulfone, and p-aminobenzoic acid, and various aromatic diamines[J].European Polymer Journal,2002(9):1721-1729. |
[4] | Park SJ;Li K;Jin FL .Synthesis and characterization of hyper-branched polyimides from 2,4,6-triaminopyrimidine and dianhydrides system[J].Materials Chemistry and Physics,2008(2/3):214-219. |