研究了高温后ECC(经设计的水泥基复合材料)的残余力学性能.将ECC试件分别加热到不同的温度(200、400、600和800℃),保持不同的恒温时间(0.5、1和2h).结果表明,试件自然冷却后受压,200℃除外,发现ECC的强度和刚度随温度和恒温时间增加而降低.采用MIP(压汞)试验测试试件的孔结构,发现试件总孔隙率和平均孔径随温度和恒温时间的增加而增加(200℃除外),这很好地解释了火后ECC试件力学性能的变化.

参考文献

[1] Victor C.Li;Shuxin Wang;Cynthia Wu .Tensile strain-hardening behavior of polyvinyl alcohol engineered cementitious composite(PVA-ECC)[J].ACI materials journal,2001(6):483-492.
[2] Li V C .On engineered cementitious composites (ECC)[J].Journal of Advanced Concrete Technology,2003,1(03):215-230.
[3] Li V C;Wu C;Wang S et al.Interface tailoring for strain-hardening polyvinyl alcohol-engineered cementitious composite (PVA-ECC)[J].ACI MATERIALS JOURNAL,2002,99(05):463-472.
[4] Kunieda M;Rokugo K .Recent progress on HPFRCC in Japan required performance and applications[J].J of Advan Con Tech,2006,4(01):19-33.
[5] Michael D. Lepech;Victor C. Li .Application of ECC for bridge deck link slabs[J].Materials and structures,2009(9):1185.
[6] 任韦波,许金余,白二雷,苏灏扬.高温后陶瓷纤维增强地聚物混凝土性能与声学损伤的关系[J].材料热处理学报,2014(03):13-19.
[7] K. Sakr;E. EL-Hakim .Effect of high temperature or fire on heavy weight concrete properties[J].Cement and Concrete Research,2005(3):590-596.
[8] Mustafa Sahmaran;Mohamed Lachemi;Victor C. Li .Assessing Mechanical Properties and Microstructure of Fire-Damaged Engineered Cementitious Composites[J].ACI materials journal,2010(3):297-304.
[9] Mustafa Sahmaran;Erdogan Ozbay;Hasan E. Yucel .Effect of Fly Ash and PVA Fiber on Microstructural Damage and Residual Properties of Engineered Cementitious Composites Exposed to High Temperatures[J].Journal of Materials in Civil Engineering,2011(12):1735-1745.
[10] Tahir Kemal Erdem.Specimen size effect on the residual properties of engineered cementitious composites subjected to high temperatures[J].Cement & concrete composites,2014:1-8.
[11] Sammy Yin Nin Chan;Xin Luo;Wei Sun .Effect of high temperature and cooling regimes on the compressive strength and pore properties of high performance concrete[J].Construction and Building Materials,2000(5):261-266.
[12] Recommendations for design and construction of high performance fiber reinforced cement composite with multiple fine cracks (in Japanese)[S].
[13] ASTM C109/C109M-12[Z].
[14] N.R. Short;J.A. Purkiss;S.E. Guise .Assessment of fire damaged concrete using colour image analysis[J].Construction and Building Materials,2001(1):9-15.
[15] Sarshar R;Khoury G A .Material and environmental factors influencing the compressive strength of unsealed cement paste and concrete at high temperatures[J].Magazine of Concrete Research,1993,45(162):51-61.
[16] Dias W P S;Khoury G A;Sullivan P J E .Mechanical properties of hardened cement paste exposed to temperatures up to 700 ℃ (1292F)[J].ACI MATERIALS JOURNAL,1990,87(02):160-166.
[17] Khoury G A .Compressive strength of concrete at high temperatures:a reassessment[J].Magazine of Concrete Research,1992,44(161):291-309.
[18] Tailor H F W.Cement Chemistry[M].New York.Academic Press,1990
[19] Gai-Fei Peng;Zhi-Shan Huang .Change in microstructure of hardened cement paste subjected to elevated temperatures[J].Construction and Building Materials,2008(4):593-599.
[20] Rostasy F S;Weiβ R;Wiedemann G .Changes of pore suucture of cement mortars due to temperature[J].Cement and Concrete Research,1980,10(02):157-164.