对湿化学法制备的SiO/3Y-TZP包裹复合粉体进行了热压烧结研究,并利用X射线衍射和透射电镜表征了烧结体的物相和显微结构.在低于1300℃,复合粉体发生瞬时粘性烧结,材料密度迅速提高;随着烧结温度的升高,SIO和ZrO发生反应生成ZrSiO.在1500℃热压条件下,制备了平均晶粒尺寸为350nm的ZrSiO/3Y-TZP细晶复相材料.我们认为,在烧结过程中形成的第二相ZrSiO,特别是SiO包裹层对抑制基体晶粒长大起主要作用.

3Y-TZP powder coated with SiO2 layer, prepared by the wet chemical method, was hot-pressed to fine-grained ZrSiO4/3Y-TZP composite. The phases and
microstructure of the sintering bodies were characterized by X-ray diffraction and TEM. Below 1300℃, the coated powder was sintered to higher density
by means of transient viscous sintering. With increasing temperature, SiO2 reacted with ZrO2 to form ZrSiO4. ZrSiO4/3Y-TZP ceramic with an average
grain size of 350nm was obtained when the coated powder was hot-pressed at 1500℃ for 1h. It was suggested that SiO2 layer made greater contributions to the
formation of the fine-grained ZrSiO4/3Y-TZP composite.

参考文献

[1] 郭景坤(GUO Jing-Kun). 无机材料学报(Journal of Inorganic Materials),1995, 10 (1): 27--31.
[2] Sacks M D, et al. J. Am. Ceram. Soc., 1991, 74: 2428--2432.
[3] Shiwei Wang , et al. Mater. Lett., 1996, 28: 43--46.
[4] 施鹰,高性能锆英石基复相陶瓷制备科学的研究. [博士论文]. 上海: 中国科学院上海硅酸盐研究所, 1995.
[5] 张宗涛, 等. 材料科学进展,1993, 7: 546--552.
[6] Phase Diagrams for Ceramists, Fig. 2388.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%