采用扫描电镜结合慢应变拉伸试验研究了表面机械处理(喷砂和砂轮盘打磨)对5083铝合金的表面形貌和拉伸性能的影响.结果表明:5083铝合金经表面机械处理后,出现了一定程度的损伤(表层产生了裂纹),从而使其拉伸时断裂时间缩短和伸长率降低,其中表面喷砂后,伸长率降低了9.9%,表面打磨后,伸长率降低了13.5%.