介绍了一种一步法制备碳化钨(WC)的新方法,以钨酸钠为原料,通过碳纳米管模板和载体制备小颗粒钨酸,制备出钨酸和碳黑的混合物作为反应前驱体,分别以H2和N2作为还原及保护气体合成WC,当合成温度高于800℃,反应前反应管内抽成真空,并在反应管内通入氢气和氮气流时,WO3首先被还原为W,接下来W被还原为W2C,最后,W2C被还原为最终产物WC.实验过程中通过调节气氛和温度2个重要反应条件,探索出了控制WC形貌及大量制备的方法,为WC的低成本及可控制备提供了新的途径.

参考文献

[1] Delanoe A;Bacia M;Pauty E;Lay S;Allibert CH .Cr-rich layer at the WC/Co interface in Cr-doped WC-Co cermets: segregation or metastable carbide?[J].Journal of Crystal Growth,2004(1/2):219-227.
[2] Hu FP;Cui GF;Wei ZD;Shen PK .Improved kinetics of ethanol oxidation on Pd catalysts supported on tungsten carbides/carbon nanotubes[J].Electrochemistry communications,2008(9):1303-1306.
[3] Christian JB;Smith SPE;Whittingham MS;Abruna HD .Tungsten based electrocatalyst for fuel cell applications[J].Electrochemistry communications,2007(8):2128-2132.
[4] Zhao ZZ;Fang X;Li YL;Wang Y;Shen PK;Xie FY;Zhang X .The origin of the high performance of tungsten carbides/carbon nanotubes supported Pt catalysts for methanol electrooxidation[J].Electrochemistry communications,2009(2):290-293.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%