为了改善硅微粉与不饱和树脂体系的亲和力,减少人造石英石板材加工过程中的树脂用量,采用改性聚硅氧烷在硅微粉的球磨过程中对其进行表面改性,并通过吸油值、悬浮体粘度及渗透时间对改性效果进行评价.结果表明,在改性聚硅氧烷用量为3.5‰时,改性硅微粉的吸油值较低、亲油性较好且与不饱和聚酯树脂的相容性最好.
In order to improve the affinity between silica powder and UP and to reduce the amount of resin dur-ing artificial stone processing,the silica powder was modified with modified polysiloxane in the process of grinding. Oil absorption,suspension viscosity and penetration time were used to characterize the modification effects. The re-sults showed that when the dosage of modifier reached to 3. 5‰,the modified quartz powder had the lower oil-ab-sorbed value,better lipophilicity and best compatibility with unsaturated polyester.
参考文献
[1] | 汪奇林;马洋洋;晏辉.人造石英石生产与安装工艺[J].石材,2015(6):11-19. |
[2] | 卢英常;张跃英.硅微粉的用途及生产技术[J].中国非金属矿工业导刊,2009(4):40-43. |
[3] | 张晓莹 .改性二水石膏/二氧化硅复合材料在树脂基人造大理石中的应用研究[D].武汉理工大学,2008. |
[4] | 王传虎;葛金龙;曾小剑.超细硅微粉表面改性的研究[J].非金属矿,2009(4):14-16. |
[5] | 李金涛;林金辉.粉石英表面改性及其效果的表征[J].非金属矿,2004(3):16-17,42. |
[6] | 陈泉水.粉石英表面改性及其作用研究[J].非金属矿,2001(02):15-17. |
[7] | 林红娇;晏泓;王亓杰;魏丽乔;许并社.硅烷偶联剂对金属氢氧化物粉体的机械球磨改性[J].中国粉体技术,2011(4):36-40. |
[8] | 余志伟.改性石英填料的性能及评价方法[J].矿物学报,2001(03):508-510. |
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%