采用差热分析仪及XRD衍射仪确定了高炉渣纤维的玻璃化转变温度、开始析晶温度及析晶相,并在此基础上结合Matusita-sakka方程研究析晶动力学,获得析晶动力学参数.结果表明:不同升温速率条件下高炉渣纤维的玻璃化转变温度为707~721℃,开始析晶温度为847~879℃;但热处理条件下高炉渣纤维的析晶温度700℃,主要是由于不同升温速率下造成温度滞后,同时随着温度的提高及在此温度长期作用下析出的主晶相为黄长石,以及少量钙长石和透辉石.高炉渣纤维晶体的生长因子m为3,表明晶体以三维方式生长,且析晶活化能约为347.287 kJ·mol-1.
参考文献
[1] | Brane Sirok;Benjamin Bizjan;Alen Orbanic.Mineral wool melt fiberization on a spinner wheel[J].Chemical Engineering Research & Design: Transactions of the Institution of Chemical Engineers,20141(1):80-90. |
[2] | I. Gnip;S. Vaitkus;S. Vejelis.An estimated prediction of the deformability of mineral wool (MW) slabs under long-term compressive stress[J].Construction and Building Materials,2013Jan.(Jan.):675-680. |
[3] | Bajcar T;Blagojevic B;Sirok B;Dular M.Influence of flow properties on a structure of a mineral wool primary layer[J].Experimental Thermal and Fluid Science: International Journal of Experimental Heat Transfer, Thermodynamics, and Fluid Mechanics,20072(2):440-449. |
[4] | 李荣缇;潘伟.非晶态莫来石纤维析晶动力学的研究[J].材料导报,2001(9):68-71. |
[5] | 温广武;雷廷权;周玉.不同形态石英玻璃的析晶动力学研究[J].材料科学与工艺,2001(1):1-5. |
[6] | 邢建申;王树彬;张跃.石英纤维析晶行为[J].复合材料学报,2006(6):75-79. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%