The effects of spinning deformation and subsequent heat treatments on the mechanical properties and microstructure of 18Ni Co-free Maraging steel (T250) tube were evaluated comparatively with the perform. An obvious radial shrinkage is detected in spun tubes after heat treatment and the magnitude of the shrinkage induced by solution treatment is almost the same as that by aging. Plastic deformation during spinning elongated the grains severely in the direction of metal flow. The solution treatment resulted in a drastically refined grain and recrystallised microstructure, removing the effect of plastic deformation, relieving the tangential residual stress and strain and improving hardness. Subsequent aging obtained a tempered microstructure, enhancing hardness values strikingly for precipitation strengthening. XRD (X-ray diffraction) analysis indicated that the reversed austenite formed in a plate-like along the grain boundaries and the volume fraction of austenite in spun tube was more than double that in the preform. These results imply that the residual stress and stain induced by spinning process and reversed austenite forming during aging might have the similar contribution to the radical shrinkage.
参考文献
[1] | Vasudevan V K;Kim S J;Wayman C M .Precipitation Reactions and Strengthening Behavior in 18wt pct Nickel Maraging Steels[J].Metallurgical Transactions,1990,21A(10):2655. |
[2] | Pereloma E V;Shekhter A;Miller M K et al.Ageing Behaviour of an Fe-20Ni-1.8Mn-1.6Ti-0.59A1(wt%)Maraging Alloy:Clustering,Precipitation and Hardening[J].Acta Materialia,2004,52(19):5589. |
[3] | R. TEWARI;S. MAZUMDER;I. S. BATRA .PRECIPITATION IN 18 WT Ni MARAGING STEEL OF GRADE 350[J].Acta materialia,2000(5):1187-1200. |
[4] | Sha W;Cerezo A;Smith G D W .Phase Chemistry and Precipi- tation Reactions in Maraging Steels:Part Ⅳ.Discussion and Conclusions[J].Metallurgical and Materials Transactions,1993,24A(06):1253. |
[5] | O. Music;J. M. Allwood;K. Kawai .A review of the mechanics of metal spinning[J].Journal of Materials Processing Technology,2010(1):3-23. |
[6] | Prakash R;Singhal R P .Shear Spinning Technology for Manu facture of Long Thin Wall Tubes of Small Bore[J].Journal of Materials Processing Technology,1995,54(1-4):186. |
[7] | Rauch G C;Daga R L;Radcliffe S V et al.Volume Expansion,Pressure Effects,and the Strength Differential in As- Quenched Iron-Carbon Martensite[J].Metallurgical and Materials Transactions,1975,6A(11):2279. |
[8] | Shibata A;Yonezawa H;Yabuuchi K et al.Relation Between Martensite Morphology and Volume Change Accompanying fcc to bcc Martensitic Transformation in Fe-Ni-Co Alloys[J].Materials Science and Engineering,2006,438-440A:241. |
[9] | Martin J W.Micromechanisms in Particle Hardened Alloys[M].Cambridge:Cambridge University Press,1980 |
[10] | Gur C H;Arda E B .Effect of Tube Spinning and Subsequent Heat Treatments on Strength,Mierostructure and Residual Stress State of AISI/SAE Type 4140 Steel[J].Materials Science and Technology,2003,19(11):1590. |
[11] | Rack H J .Age Hardening Grain Size Relationships in 18Ni Maraging Steels[J].Mater Sciand Eng,1978,34(03):263. |
[12] | Pardal JM;Tavares SSM;Fonseca MP;Abreu HFG;Silva JJM .Study of the austenite quantification by X-ray diffraction in the 18Ni-Co-Mo-Ti maraging 300 steel[J].Journal of Materials Science,2006(8):2301-2307. |
[13] | C. R. Shamantha;R. Narayanan;K. J. L. Iyer;V. M. Radhakrishnan;S. K. Seshadri;S. Sundararajan;S. Sundaresan .Microstructural changes during welding and subsequent heat treatment of 18Ni (250-grade) maraging steel[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2000(1):43-51. |
[14] | Moyer J M;Ansell G S .The Volume Expansion Accompan ying the Martensite Transformation in Iron-Carbon Alloys[J].Metallurgical and Materials Transactions,1975,6A(09):1785. |
[15] | Sinha P P;Tharian K T;Sivakumar D .Effect of Solution Treatment Temperatures on Microstructure,Tensile and Fracture Properties of Co-Free 18Ni Maraging Steel[J].Steel Research International,1994,65(11):494. |
[16] | P. P. Sinha;K. T. Tharian;K. Sreekumar;K. V. Nagarajan;D. S. Sarma .Effect of aging on microstructure and mechanical properties of cobalt free 18% Ni(250 grade) maraging steel[J].Materials Science and Technology: MST: A publication of the Institute of Metals,1998(1):1-9. |
[17] | Vanderwalker D M .The Precipitation Sequence of Ni3Ti in Co-Free Maraging Steel[J].Metallurgical and Materials Transactions,1987,18A(07):1191. |
- 下载量()