The nondendritic semi-solid slurry preparation of high chromium cast iron Cr20Mo2 has been studied in this paper. The experiments show that the proeutectic austenitic particles are more spherical under a larger stirring power condition, even if the stirring time is shorter, while the proeutectic austenitic particles are not very much spherical under a smaller stirring power condition and some proeutectic austenitic dendrites also exist, even if the stirring time is very long. The experiments also show that when stirred for 5 6 minutes under the test condition, the semi-solid slurry with 40vol. %-50vol. % solid fraction and spherical proeutectic austenite in the size of 50-80μm can be obtained.

参考文献

[1] M C Flemings .[J].Metallurgical and Materials Transactions,1991,22A(05):957.
[2] M Garat;S Blais;A K Bhasin;J J Moore,K P Young and S Midson.[A].Golden, Colorado, USA, June 23-25,1998:199.
[3] P Eisen;K Young;G L Chiarmetta;M Rosso.The 6th Int. Conf. on Semi-Solid Processing of Alloys and Composites[M].Politecnico Di Torino,Turin,Italy,Sept. 27-29,2000:41.
[4] K P Young;R G Riek;M C Flemings .[J].Metals and Technology,1979,6(06):130.
[5] P Kapranos;D H Kirkwood;C M Sellars;eds D H Kirkwood and P Kapranos (.The 4th Int. Conf. on Semi-Solid Processing of Alloys and Compositions[C].The Universiy of Sheffield, England, June19-21,1996:306.
[6] K E Blazek;J E Kelly;N S Pottorethe .[J].ISIJ International,1995,35(06):813.
[7] 毛卫民,赵爱民,崔成林,孙峰,郑承利,钟雪友.AlSi7Mg合金半固态连铸坯料和组织形成研究[J].金属学报,2000(05):539-544.
[8] W M Mao;A M Zhao;Y J Li;X Y Zhong .[J].Science and Technology of Advanced Materials,2001,29(01):97.