采用机械合金化法制粉、液相烧结和致密化处理工艺,制备了低质量分数的Mo-Cu合金.通过X射线衍射和扫描电镜对Mo-Cu复合粉末形貌、液相烧结和变形加工后合金显微组织进行了分析,研究了各种工艺参数对Mo-Cu合金致密性、拉伸强度和延伸率的影响.结果表明,采用高能球磨机械合金化和液相烧结,可获得相对密度高达98.2%的Mo-Cu合金, 再经致密化变形加工处理后,可获得全致密的Mo-Cu合金,在40%变形率的条件下,拉伸强度可达到569MPa,延伸率为6.3%.

参考文献

[1] Suryanarayana C .[J].Materials Science,2001,46:181-184.
[2] Suryanarayana C et al.[J].Materials Today,2005,11:62.
[3] 刘海彦,李增峰,汤慧萍,高广瑞,黄原平.机械合金化制备钼铜复合材料[J].功能材料,2004(z1):3294-3296.
[4] Alam S N .[J].Materials Science and Engineering,2006,433:161-168.
[5] Maneshian M H;Simchi A .[J].Journal of Alloys and Compounds,2008,463:153-159.
[6] Ivanov E Y;Suryanarayana C;Bryskin B D .[J].Materials Science and Engineering,1998,251:255-261.
[7] Martinez V;Aguilar C;Marin J et al.[J].Materials Letters,2007,61:929-933.
[8] Aguilar C;Marin J;Ordonez S et al.[J].Materials Science and Engineering,2007,464:288-294.
[9] John L. Johnson;Randall M. German .Powder metallurgy processing of Mo-Cu for thermal management applications[J].International Journal of Powder Metallurgy,1999(8):39-48.
[10] 南海,曲选辉,方玉诚,何新波.电子封装用注射成形Mo/Cu合金烧结工艺的研究[J].粉末冶金工业,2004(06):1-5.
[11] 张朝晖,王富耻,李树奎.静液挤压钨合金的显微组织与力学性能[J].中国有色金属学报,2001(z1):88-91.
[12] 张朝晖,王富耻,李树奎.钨合金的静液挤压变形强化[J].兵工学报,2002(02):224-227.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%