研究了不同烧结温度和保温时间下烧结对银膜附着力和方阻的影响,用扫描电镜观察烧结后银膜的形态。结果表明,在850℃烧结保温40 s得到的银膜性能较优,银膜的附着力和方阻分别为3.193 N和4.16 m?/□。

The effects of different sintering temperatures and holding time on the adhesion force and square resistance of the silver film were studied through a series of experiments, and the morphology of the sintered silver film was observed by SEM. The results showed that the silver film sintered at 850℃ for 40 seconds has better properties after sintering. The adhesion force and square resistance of the silver film are 3.193 N and 4.16 m?/□, respectively.