由NiCl2、NaBH4等组成的微乳液体系发生氧化还原反应制备NiO纳米棒前驱物,在熔融盐环境中860℃焙烧2.5h前驱体发生氧化反应,成功地制备了NiO纳米棒,用透射电子显微镜、X射线衍射对NiO纳米棒进行了表征.