高级检索

对T/P92、T/P122、S30432(Super 304H)、S31042(HR3C)、9Cr3W3Co等先进锅炉钢的性能进行了综合评述,对比分析了这几种钢管及其焊接接头的持久强度、抗腐蚀性能和常规力学性能数据,采用等温线法和Larson-Miller法外推了这些锅炉钢的10万h持久强度,探讨了这几种钢管许用应力的设定及在工程设计和应用的问题.

The important properties of some boiler steels such as T/P92, T/P122, S30432 (Super 304H), S31042 (HR3C) and NIMS-9Cr3W3Mo were critically reviewed. The creep rupture strength, corrosion resistance and conventional strength of these steels and their welding parts were carefully compared and isothermal curve method and Larson-Miller method were used to reasonably extrapolate creep rupture strengths of these steels after 10~5 h service. Meanwhile, allowable stress of these steel tubes and pipes and associated engineering concerns were also discussed.

参考文献

[1] 刘正东,程世长,包汉生,杨钢,干勇.超超临界火电机组用锅炉钢技术国产化问题[C].中国金属学会特钢分会、特钢冶炼学术委员会2008'年会论文集,2008:132-141.
[2] 杨富;李为民;任永宁.超(超)临界锅炉用新型铁素体耐热钢的现状与发展[A].苏州:电力行业电力锅炉压力容器安全监督管理委员会,2005:30.
[3] 束国刚;赵彦芬;张路.超(超)临界锅炉用新型奥氏体耐热钢的现状与发展[A].苏州:电力行业电力锅炉压力容器安全监督管理委员会,2005:37.
[4] 刘正东;杨素宝;程世长 等.超超临界火电机组用钢性能数据库管理系统V1.0[P].中国,2008SRBJ2578,2008-08-22.
[5] 太田定雄;张善元;张绍林.铁素体系耐热钢-向世界前沿不懈攀登的研究与开发[M].北京:冶金工业出版社,2003
[6] 范长信.国内外超超临界机组材料及焊接研究资料汇编[M].西安:西安热工研究院,2004
[7] Shaju K. Albert;Masayuki Kondo;Masaaki Tabuchi .Improving the Creep Properties of 9Cr-3W-3Co-NbV Steels and their Weld Joints by the Addition of Boron[J].Metallurgical and Materials Transactions, A. Physical Metallurgy and Materials Science,2005(2):333-343.
[8] Emad EL-KASHIF;Kentaro ASAKURA;Koji SHIBATA .Effects of Nitrogen in 9Cr-3W-3Co Ferritic Heat Resistant Steels Containing Boron[J].ISIJ International,2002(12):1468-1476.
[9] Akio Sasada .Precipitates and Precipitation Site in Creep-Ruptured 9Cr-3W-3Co-V-Nb Steel[J].Materials and Processes,2001,13(06):1217.
[10] GB/T 2039-1997.GB/T 2039-1997.金属拉伸蠕变及持久试验方法[S].
[11] ISO 204-1997.ISO 204-1997.Metallic Materials-Uniaxial Creep Testing in Tension-Methods of Test[S].
[12] BS EN 10291-2000.BS EN 10291-2000.Metallic Materials-Uniaxial Creep Testing in Tension-Methods of Test[S].
[13] JIS Z2271-1999.JIS Z2271-1999.Metallic Materials-Uniaxial Creep Testing in Tension-Methods of Test[S].
[14] 陈明浩;史柏海;章应霖 .热强钢持久强度的统计特性及其寿命评定[J].华中电力,1998,11(03):5.
[15] 张建强,赵海燕,鹿安理,章应霖,陈明浩.耐热钢持久强度的统计特性及其在寿命评估中的应用[J].机械强度,2004(06):701-705.
[16] 徐自立.高温金属材料的性能、强度设计及工程应用[M].北京:化学工业出版社,2006
[17] 周顺深.用持久强度计算高温部件剩余寿命的不可靠性[J].华东电力,1995(03):1.
[18] Walter Bendick;Jean Gabrel .Assessment of creep rupture strength for the new martensitic 9 percent Cr steels E911 and T/P92[J].Materials at High Temperatures,2008(3):139-148.
[19] DL/T 5054-1996.DL/T 5054-1996.火力发电厂汽水管道设计技术规定[S].
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%