在Gleeble-3500型热模拟试验机上对高碳钢SWRH72A盘条进行了不同条件下的氧化试验,采用OM、SEM和XRD等技术对氧化皮形貌、厚度和结构进行表征.结果表明,高碳钢氧化皮一般呈Fe1-yO和Fe3O4两层结构,其厚度与氧化温度的关系近似符合Arrhenius方程,并随氧化时间呈抛物线型增长,氧化皮中Fe1-yO/Fe3O4厚度比与氧化温度和氧化时间的关系与厚度的变化规律基本一致.机械剥离试验结果表明,当氧化皮较薄时(<27μm),机械剥离率随厚度近似成线性增长,而当氧化皮厚度达到一定程度后(≥27μm),机械剥离率不再增加,基本保持不变.
参考文献
[1] | Tominaga J;Wakimoto K;Mori T et al.Manufacture of wire rods with good desealing property[J].Transactions ISlJ,1982,22:646-656. |
[2] | Confente M;Geneve D;Resiak B et al.Effects of mechanical deltealing On the surfaee of low carbon wire rod for drawing or cold heading[J].Wire Journal Intemational,1995,28:238-242. |
[3] | Parusov V V;Savyuk A N;Sychkov A B et al.Study of the possibilities for maximizing scale removal from wire rod before drawing[J].METALLURGIST,2004,48:292-297. |
[4] | Chen R Y;Yuen W Y D .Review of the high-temperature oxidadon of iron and carbon steels in air or oxygen[J].Oxidation of Metals,2003,59(5/6):433-468. |
[5] | Chen R Y;Yuen W Y D .Oxide-scale structures formed on commercial hot-rolled gteel strip and their formation mechanisms[J].Oxidation of Metals,2001,56(1/2):89-118. |
[6] | R. V. Chen;W. V. D. Vuen .A Study of the Scale Structure of Hot-Rolled Steel Strip by Simulated Coiling and Cooling[J].Oxidation of Metals,2000(5/6):539-560. |
[7] | Sun W H;Tieu A K;Jiang Z Y et al.High temperature oxide scale characteristie of low carbon steel in hot rolling[J].Journal of Materials Processing Technology,2004,155-156:1307-1312. |
[8] | Basabe VV;Szpunar JA .Growth rate and phase composition of oxide scales during hot rolling of low carbon steel[J].ISIJ International,2004(9):1554-1559. |
[9] | BK-Spec:GA-03-17.Descalability of high carbon wire rod-quick test[S].,2003. |
[10] | 李铁藩.金属高温氧化和热腐蚀[M].北京:化学工业出版社,2003:168-173. |