采用简单方便的方法制备了钙钛矿型催化剂La0.8K0.2Cu0.05Mn0.95O3,用程序升温反应的方法评价催化剂同时去除NOx和碳烟的性能,利用XRD、BET和SEM研究煅烧温度对其结构的影响,进而从物理角度分析催化剂性能的影响因素.结果表明,随着煅烧温度的升高,催化剂的晶型更加完美,比表面积和平均孔径都下降,内部的微孔逐渐减少.结合程序升温反应可知,最有利于同时催化去除NOx和碳烟的催化剂的平均孔径为17nm左右.
参考文献
[1] | Libby W F .[J].Science,1971,171(3970):499-500. |
[2] | Voorhoeve R J H;Remeika J P;Freeland P E .[J].Science,1972,177(4046):353-354. |
[3] | Yoshida K;Makino S;Sumiya S et al.[J].Plant Physical,1989,89:1331-1336. |
[4] | Setiabudi A;Makkee M;Moulijn J A .[J].Applied Catalysis B:Environmental,2003,42(01):35-45. |
[5] | Carrascull A D;Lick I N;Ponzi E et al.[J].Catalysis Communications,2003,4:124-128. |
[6] | Long XL;Xin ZL;Wang HX;Xiao WD;Yuan WK .Simultaneous removal of NO and SO2 with hexamminecobalt(II) solution coupled with the hexamminecobalt(II) regeneration catalyzed by activated carbon[J].Applied Catalysis, B. Environmental: An International Journal Devoted to Catalytic Science and Its Applications,2004(1):25-32. |
[7] | Teraoka Y;Kanada K;Kagawa S .[J].Applied Catalysis B:Environmental,2001,34(01):73-78. |
[8] | Teraoka Y;Nakano K;Kagawa S et al.[J].Applied Catalysis B:Environmental,1995,5(03):181-185. |
[9] | Teraoka Y;Nakano K;Shangguan W F et al.[J].Catalysis Today,1996,27:107-113. |
[10] | Shangguan W F;Teraoka Y;Kagawa S .[J].Applied Catalysis B:Environmental,1996,8(02):217-227. |
[11] | Shangguan W F;Teraoka Y;Kagawa S .[J].Applied Catalysis B:Environmental,1997,12(2-3):237-247. |
[12] | Shangguan W F;Teraoka Y;Kagawa S .[J].Applied Catalysis B:Environmental,1998,16(02):149-154. |
[13] | 刘光辉,黄震,上官文峰,阎存仙.同时催化去除柴油机微粒和NOx的试验研究(1)[J].内燃机学报,2003(01):40-44. |
[14] | Pitchon V;Fritz A .[J].Applied Catalysis B:Environmental,1997,13(01):1-25. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%