本文采用传统熔融方法制备了BaO-B2O3系列基础玻璃(BaO-B2O3、BaO-B2O3-0.1Al2O3、BaO-B2O3-0.2SiO2、BaO-B2O3-0.4TiO2)(mol%),通过对基础玻璃进行表面修饰处理,控制表面析晶条件,获得了含有沿α轴择优取向生长BBO微晶的透明BaO-B2O3系列表面析晶玻璃陶瓷.

Optically transparent BaO-B2O3 (in mol%) system glass was successfully prepared by theconventional melting and quenching technique. After surface controlled crystallization, the grAlN-oriented transparent β-BaB2O3 (BBO) surface crystallized glass -ceramics were prepared. Inaddition, the polar-oriented growth kinetics of BaO-B2O3 glass was discussed.