The method of examining micro-pores in sulphoaluminate MDF cement by means of the Positron Annihilation Technique (PAT) was discussed.The results show that the intensity I2 of positrons annihilation with moderate life-span (τ2≈330Ps) increases regularly with the addition of the numbers of micro-pores (less than 250(A)). Therefore, the value of I2 may be used to opitomize the compactness and integrity of the MDF cement structure. At the same time, the experiment result of PAT was compared with that of Mercury Intrusion Porosimeter (MIP).
参考文献
[1] | Zhang Xiaowen.Struture Base of Solid Materials[M].北京:中国建筑工业出版社,1980:46. |
[2] | N MCN .Alford and J D Birchall[J].Journal of Materials Science,1985,20:37-45. |
[3] | Huang Congyun.The Studies of Advanced SAC-MDF Cement and Its Coupling Stabilizing Toughening Mechanism[M].武汉:武汉科技大学,2000 |
[4] | SONG Shao-min,LIU Juan-hong,ZHANG XI-qing.Performance of the Cement Matrix Composite Material With Rubber Powder[J].武汉理工大学学报(材料科学版)英,2004(01):77-80. |
[5] | Huang Cong-yun,YUAN Run-zhang,LONG Shi-zong.The Pore Structure and Hydration Performance of Sulphoaluminate MDF Cement[J].武汉理工大学学报(材料科学版)英,2004(01):83-85. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%