采用表面机械研磨处理技术(Surface mechanical attrition treatment,SMAT)在工业纯Ti的表面制备出一层厚度约30μm纳米结构表层,最表层的平均晶粒尺寸约30 nm.随后在常温(25℃)下对其进行双氧水及400℃煅烧处理,并采用X射线光电子能谱(XPS)等手段进行了逐层结构分析.结果表明,SMAT Ti表面与粗晶Ti表层形成的氧化层结构存在明显差别.

参考文献

[1] 冯波,翁杰,屈树新,鲁雄,汪建新.医用钛表面纳米结构化改性[J].稀有金属材料与工程,2007(10):1693-1697.
[2] Liu XY;Chu PK;Ding CX .Surface modification of titanium, titanium alloys, and related materials for biomedical applications[J].Materials Science & Engineering, R. Reports: A Review Journal,2004(3/4):49-121.
[3] Thomsen P;Larsson C;Ericson LE;Sennerby L;Lausmaa J;Kasemo B .Structure of the interface between rabbit cortical bone and implants of gold, zirconium and titanium[J].Journal of Materials Science. Materials in Medicine,1997(11):653-665.
[4] Lu K;Lu J .[J].Journal of Materials Science and Technology,1999,15:193.
[5] Lu K Lu J .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2004,375-377:38.
[6] Wen M;Liu G;Gu JF;Guan WM;Lu J .The tensile properties of titanium processed by surface mechanical attrition treatment[J].Surface & Coatings Technology,2008(19):4728-4733.
[7] Wen M;Gu JF;Liu G;Wang ZB;Lu J .Formation of nanoporous titania on bulk titanium by hybrid surface mechanical attrition treatment[J].Surface & Coatings Technology,2007(14):6285-6289.
[8] Wen, M;Gu, JF;Liu, G;Wang, ZB;Lu, J .Surface evolution of a gradient structured Ti in hydrogen peroxide solution[J].Applied Surface Science,2008(9):2905-2910.
[9] Carley A F et al.[J].Journal of the Chemical Society,Faraday Transactions,1987,83:351.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%