高级检索

At different annealing temperatures, the saturation magnetostrictions and the correlation between the permeability μi and the temperature T(μi-T curves) of the Co66Fe4Mo2Si16B12 alloy were investigated using a small-angle magnetization tester and core tester. The experimental results showed that the μi-T curves had different shapes at different ranges of annealing temperature; the permeability μi of the alloy improved with increasing the annealing temperatures below 460℃; when the alloy was annealed above 480℃, the poor magnetic properties were considered to be caused by larger saturation magnetostriction.