高级检索

用座滴法研究了高真空下Zr41.25Ti13.75Ni10Cu12.5Be22.5(原子百分数,下同)熔体在W上的润湿行为及界面相互作用,并用浸渗法制备了W丝增强的Zr41.25Ti13.75Ni10Cu12.5Be22.5块状非晶复合材料.结果表明:在1053 K~1173 K之间,Zr41.25Ti13.75Ni10Cu12.5Be22.5熔体与W具有较好的润湿性.润湿温度升高会显著降低平衡接触角,并加速熔体的铺展,但也会增大W的溶解量.继续升高温度对平衡接触角和达到平衡接触角所需时间的影响很小.好的润湿性和快的铺展速率为制备W丝增强的Zr41.25Ti13.75Ni10Cu12.5Be22.5块状非晶复合材料选择合理的工艺参数提供了较大的自由空间.

参考文献

[1] Asthana R. .Reinforced cast metals - Part II Evolution of the interface [Review][J].Journal of Materials Science,1998(8):1959-1980.
[2] Mortensen A .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,1991,135(03):1.
[3] Naiditch J V .[J].Prog Surf Membrane Sci,1981,14:353.
[4] Choi Y H;Busch R;K(o)ster U et al.[J].Acta Materialia,1999,47(09):2455.
[5] Conner R D;Dandliker R B;Johnson W L .[J].Acta Materialia,1998,46(16):6089.
[6] Dandliker R B;Conner R D;Johnson W L .[J].Journal of Materials Research,1998,13(10):2896.
[7] 邱克强,王爱民,张海峰,乔东春,丁炳哲,胡壮麒.钨丝增强ZrAlNiCuSi块体非晶复合材料及其塑性行为[J].金属学报,2002(10):1091-1096.