对260BD冷轧烘烤硬化钢镀锌板进行点焊试验,研究了焊接工艺参数(焊接时间及焊接电流)对焊点熔核尺寸及拉剪性能的影响,建立了点焊工艺窗口,并分析了焊点不同区域的微观组织及硬度.结果表明:随着焊接电流和焊接时间的增加,焊点的最大拉剪力和熔核尺寸均增大,但当电流过大而发生飞溅时,焊点的最大拉剪力和熔核尺寸将减小,此外焊点不同区域微观组织的差异导致了焊点硬度分布的不均匀性.

参考文献

[1] Doo-Hwan Kim;Ho-Kyung Kim.Fatigue strength evaluation of cross-tension spot weld joints of cold rolled mild steel sheet[J].Materials & Design,20098(8):3286-3290.
[2] De-Guang Shang.Measurement Of Fatigue Damage Based On The Natural Frequency For Spot-welded Joints[J].Materials & design,20094(4):1008-1013.
[3] 魏世同;吕冬;刘仁东;林利.电极端面尺寸对IF钢镀锌板点焊性能的影响[J].鞍钢技术,2014(3):23-27.
[4] Xin Sun;Elizabeth V. Stephens;Mohammad A. Khaleel.Effects of fusion zone size and failure mode on peak load and energy absorption of advanced high strength steel spot welds under lap shear loading conditions[J].Engineering failure analysis,20084(4):356-367.
[5] S. T. Wei;D. Lv;D. Liu.Similar and dissimilar resistance spot welding of advanced high strength steels: welding and heat treatment procedures, structure and mechanical properties[J].Science and Technology of Welding and Joining,20145(5):427-435.
[6] G. KRAUSS;S. W. THOMPSON.Ferritic microstructures in continuously cooled low- and ultralow-carbon steels[J].ISIJ International,19958(8):937-945.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%