本文主要研究含Cr2O3的硅酸锆结合SiC耐火材料的抗粉煤灰侵蚀规律,将两种不同的粉煤灰平铺在SiC耐火材料上,作用温度为1250~1450 ℃,保温时间为40小时,然后用视频光学显微镜和XRD衍射图谱来确定其显微结构和物相组成,初步实验结果表明SiC质耐火材料具有较好的抗煤灰侵蚀性能.

参考文献

[1] Donglin Chen;Chuguang Zheng;Huaichun Zhou et al.Quasi-Constant Temperature Combustion for Improving Overall Performance of a Coal-Fired Boiler[J].Combustion and Flame,2003,134(02):81-92.
[2] Donglin Chen;Chuguang Zheng .Design of Microporous Ceramic Board Based Movable Heat-Insulating Refractory Device and its Potential Merits for Coal-Fired Boilers[J].Journal of the Institute of Energy,2003,76(07):151-158.
[3] Donglin Chen;Chuguang Zheng .Experimental investigation on the feasibility of a movable heat-insulation device[J].Applied thermal engineering: Design, processes, equipment, economics,2002(17):1905-1918.
[4] Jon Wells;Gerry Riley;Jim Williamson .Interactions between coal-ash and burner quarls. Part 1: Characteristics of burner refractories and deposits taken from utility boilers[J].Fuel,2003(15/17):1859-1865.
[5] Jon Wells;Gerry Riley;Jim Williamson .Interactions between coal-ash and burner quarls. Part 2: resistance of different refractory materials to slag attack in a combustion test facility[J].Fuel,2003(15/17):1867-1873.
[6] 秦风久 .高炉用SiC砖显微结构及其抗侵蚀特征[J].东北大学学报,1994,15(05):457-446.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%