针对45圆钢热顶锻开裂问题,从宏观和微观两方面对裂纹原因进行分析,结果表明圆钢折叠缺陷是引起热顶锻裂纹的主要原因,同时局部脱碳加剧了顶锻开裂。可以通过严格执行检修和轧制制度,同时配合优化轧钢加热制度来消除热顶锻裂纹的发生。

By analyzing crack samples of hot forging for 45 round steel from both macro and micro, it can be found that the crack was mainly caused by folding, and local surface decarburization of round steel sharpened the crack of hot forging. By implementing regulations on overhaul and rolling strictly, and optimizing heating institution, the crack of hot forging could be prevented.

参考文献

[1] 吕炎.锻件缺陷分析与对策[M].北京:机械工业出版社,1983
[2] 孔祥涛,包燕平,孙彦辉,吴松巧,鲁欣武,胡文豪,金进文,郑为民.影响中、小型转炉45圆钢热顶锻合格率的冶金因素分析[C].2005中国钢铁年会论文集,2005:209-213.
[3] 翁宇庆.轧钢新技术3000问:型材分册上[M].北京:中国科学技术出版社,2005
[4] 安诚庆,张希元,张宏.冷镦钢顶锻开裂原因分析及其改进措施[J].轧钢,2003(01):66-67.