欢迎登录材料期刊网

材料期刊网

高级检索

The atmospheric corrosion of A3 steel with Na2SO4,(NH4) SO4,NH4Cl and NaCl deposited on it has been investigated at 298 K with relative humidity of (85 +/- 5) %. The results show: that A3 steel deposited by the salts corroded more and more seriously as the corrosion time went on and metal loss obeys the equation of Deltam/ A = K . t(h). FTIR, SEM and XRD were utilized to study the development and characterization of corrosion products, and the results indicate that A3 steel with the salts deposited corroded much faster than the blank samples, and the corrosion of A3 steel initialed along the deposition area of the salts.

参考文献

上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%