采用机械研磨-电场激活压力辅助合成(FAPAS)技术,快速合成了稀土Sc和Y掺杂的Mg2Si基热电材料,所得试样组织均匀、致密,试样的平均晶粒尺寸为1.5~2μcm,微量稀土元素不改变基体材料的组织形貌.分析表明两种稀土元素均在不同程度改善热电性能,其中掺杂0.427%(摩尔分数)Sc和0.173%(摩尔分数)Y的试样的综合电功率因子在378和468K分别达到未掺杂试样的2.67和2.03倍;掺杂0.173%(摩尔分数)Y的试样的热导率相对于未掺杂降低了20 %,其无量纲热电优质系数ZT相对于后者提高了1.30倍,ZTmax为0.23,明显高于未掺杂试样的0.18.
参考文献
[1] | Jun-ichi T;Hiroyasu K .[J].Physica B:Condensed Matter,2005,364:218-224. |
[2] | Jun-ichi T;Hiroyasu K .[J].Intermetallics,2007,15:1202-1207. |
[3] | Isoda Y;Nagai T;Fujiu H.Thermoelectric Properties of Sb.doped Mg2Si0.5 Sn0.5[A].Vienna,Austria,2006:406-410. |
[4] | Meng Q S;Wang L Q;Li B S.[J].Current Advancements in Molecular Medicines,2009(79-82):1639-1642. |
[5] | Meng Q S;Fan W H;Chen R X et al.[J].Journal of Alloys and Compounds,2010,492:303-306. |
[6] | Takahata K;Iguchi Y;Tanaka D et al.[J].Physical Review B,2000,19(61):12551-12555. |
[7] | Hashimoto H;Kusunose T;Sekino T .[J].Journal of Alloys and Compounds,2009,484:246-248. |
[8] | Busch G;Winkler U;Helv .[J].Physica,1954,20:1067-1072. |