用葛摆测量了a-PdCuSi合金的内耗-温度曲线,证明在该合金的Tg和Tx温度附近有两个内耗峰P1和P2.P2峰是与非晶晶化有关的内耗峰,而P1峰可能是弛豫型的内耗峰.分析了倒扭摆和Collette摆的灵敏度,阐述了这两种摆不适用于测量a—PdCuSi类合金的内耗峰.
The internal friction of the amorphous Pd77.5 Cu6.0 Si16.5 alloy (a-PdCuSi) was measured with a conventional torsion Pendulum(Ke torsion pendulum)in ascending temperatres and it was evident that there were two internal friction Peaks (p1 and p2 peaks) nea
参考文献
[1] | HEYizhen,LiXiaoguang.PhysStatSol,1987,(3)99:1152李晓光,何怡贞.物理学报,1991,40:5753SinningHRJNon-CrystSol,1989,110:1954LIXiaoguang,ZHANGYuheng,HEYizhen,JPhys.:CondensMatter,1990,2:8095KissingerHE.AnalChem,1957.29:17026SinningHRJPhysE:SoiInstrum,1986,19:8667水嘉鹏.理化检验-物理分册,1992,28(4):32 |