At first, a series of finite element method (FEM) simulation tests were used to find the critical forming conditions of hot-galvanized sheet steel during the rectangular box drawing processing when constant blank holder forces were applied. According the test results, the reasonable alteration scope of initial variable blank holder force (VBHF) wasas 1.9~2.3 T. Then, based on the test productions of blank holder force, 12 typical VBHF curves were applied to perform the simulation tests by the simulation software of DYNAFORM. The simulation test results showed that VBHF had great effects on drawing formability of hot-galvanized sheet steel during the rectangular box drawing.However, the different VBHF curves were applied to control the whole drawing and it would get great different effects. At the same tine, the VBHF had great effects on the maximum thick thinning ratio, but had little effect on the maximum thick incrassation ratio. So, reasonable application of the VBHF would greatly decrease the fractures.When the VBHF profile is taken as curve L, the best effect of drawing formability could be obtained. When curve I is used, contrary effect could be gotten. The other types of curves would cause effects between above two types of VBHF curves. Finally, the actual tests were applied to check the validity of the FEM simulation tests. The results show that the FEM simulation tests are good ways for predicting and optimizing the VBHF.
参考文献
[1] | M Ahmetoglu;T Altan .Engineering Research Center for Net Shape Manufacturing[R].Ohio State University Report No ERC/NSM-S-92-50,1992. |
[2] | Dajun HE;Yongqin WANG .[J].Mater Forming Mach,2002,37(01):41. |
[3] | Y. J. Luo;Y. Q. Zhang;D. N. He .DETERMINATION OF BLANK HOLDER FORCE IN SHEET METAL DEEP DRAWING PROCESS[J].Acta metallurgica Sinica,2003(1):31-34. |
[4] | E. J. Obermeyer;S. A. Majlessi .A review of recent advances in the application of blank-holder force towards improving the forming limits of sheet metal parts[J].Journal of Materials Processing Technology,1998(1/3):222-234. |
[5] | K Siegert;E Dannenmann;A Galeiko .[J].Annals of the CIRP,1995,44(01):251. |
[6] | Chengzhi SUN;Guanlong CHEN;Shuhui LI;Qinzhong LIN .[J].J Plast Eng,2003,10(04):6. |
[7] | D E Hardt;R C Fenn.[J].Journal of Engineering for Industry-Transactions of the ASME,1993(115):17. |
[8] | D E Hardt;R C Fenn.[J].Journal of Engineering for Industry-Transactions of the ASME,1993(115):299. |
[9] | E Siebel;H Beisswanger.[M].Carl Hanser Munich,1995 |
[10] | H B Sim;M C Boyce.[J].ASME Journal of Engineering Materials and Technology,1992(114):180. |
[11] | J Cao;M C Boyce;D E Hardlt.[J].ASME Journal of Engineering Materials and Technology,1994(294):265. |
[12] | J Cao;P Jalkh;M C Boyce;D E Hardt.IDDRG'94[C].,1994 |
[13] | W Thoma .[D].Ohio State University,1999. |
[14] | Xiaopei WANG.Stamping Handbook[M].北京:机械工业出版社,1990 |
[15] | Chinese Mechanical Engineering Society.Forging and Stamping Handbook[M].北京:机械工业出版社,2002 |
[16] | Chengzhi SUN;Guanlong CHEN;Zhongqin LIN;Weigang ZHANG .[J].J Shanghai Jiaotong Univ,2000,38(07):1086. |
[17] | Yiguo PAN;Juchen XIA;Shikun XIE.[J].Engineer,2004(01):61. |
[18] | Junxiang LEI.[J].Journal of Iron and Steel Research,2004(05):43. |
[19] | M Ahmeloglu;T Altan;G Kinzel.[J].Journal of Materials Processing Technology,1992(33):195. |
[20] | W Thoma;T Ocnoki;T Altan.[J].Journal of Materials Processing Technology,2002(98):232. |
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%