采用沉积-沉淀法制备了Au/Al2O3,探讨了预处理条件对催化剂中金颗粒的大小及其催化CO氧化性能的影响,并以XRD和TEM等手段对催化剂进行了结构表征.结果表明,还原和焙烧预处理得到的1.2% Au/Al2O3催化剂在GHSV=1.5×104 h-1时,可分别于-22和-10 ℃将空气中的1%CO完全氧化, 还原预处理所得催化剂的活性更高, 原因是催化剂中金颗粒的尺寸更小,分散度更高.
参考文献
[1] | Haruta M;Yamada N;Kobayashi T;Lijima S .[J].Journal of Catalysis,1989,115(02):301. |
[2] | Haruta M .[J].Catalysis Today,1997,36(01):153. |
[3] | Thompson D T .[J].Gold Bulletin,2001,34(02):56. |
[4] | Thompson D T .[J].Gold Bulletin,2001,34(04):134. |
[5] | Bethke GK.;Kung HH. .Selective CO oxidation in a hydrogen-rich stream over Au/gamma-Al2O3 catalysts[J].Applied Catalysis, A. General: An International Journal Devoted to Catalytic Science and Its Applications,2000(Special Issue SI):43-53. |
[6] | Ueda A;Oshima T;Haruta M .[J].Applied Catalysis B:Environmental,1997,12(2-3):81. |
[7] | Ueda A;Haruta M .[J].Applied Catalysis B:Environmental,1998,18(1-2):115. |
[8] | Seker E;Cavataio J;Gulari E;Lorpongpaiboon P Osuwan S .[J].Applied Catalysis A:General,1999,183:121. |
[9] | Shibata M;Kawata N;Masumoto T.Japan-France Seminar on Catalysis with Metal Compounds[J].Tokyo,1987:98. |
[10] | Aida T;Higuchi R;Niiyama H.[J].Chemistry Letters,1990(12):2247. |
[11] | 齐世学,邹旭华,徐秀峰,安立敦,李树本.制备条件对Au/TiO2催化CO氧化性能的影响[J].分子催化,2002(02):139-143. |
[12] | 齐世学,邹旭华,徐秀峰,安立敦,李树本,程谟杰,包信和.NO在Au/Al2O3催化剂上还原反应的TPD-MS研究[J].催化学报,2003(03):203-207. |