采用液相包裹法对Al2O3微粉进行稀土Y2O3表面改性,用挤压铸造法制备表面经稀土Y2O3改性的Al2O3/Al复合材料,并对复合材料的显微组织及界面进行观察和分析.结果表明:表面经稀土Y2O3改性的Al2O3微粉能均匀的分布于基体中,界面润湿性得以改善,复合材料组织更加均匀.拉伸性能测试表明:改性粉体对Al合金拉伸性能增强效果明显.对复合材料界面进行TEM,HREM及电子衍射分析表明,界面结合良好,界面处有Y2Al生成.EDAX分析表明界面相是钇、铝含量很高的物相;XRD图谱中也显示出Y2Al的衍射峰.

参考文献

[1] Wang Duan-Jen;Wu Shinn-Tyan .[J].Acta Metallurgica Et Materialia,1995,43(08):2917-2920.
[2] Landry K;Rado C;Eustathopoulos N .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1996,27A:3181-3186.
[3] Kobashi M;Choh T .[J].Materials Transactions,1990,31(12):1101-1107.
[4] Espie L;Drevet B;Eustathopoulos N .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1994,25A:599-605.
[5] Wang Yu-Qing;Zhou Ben-Liam .Effect of a fiber coating on the fabrication of fiber reinforced metal-matrix composites[J].Journal of Materials Processing Technology,1998(1/3):78-81.
[6] Akira Kitahara;Shigeru Akiyama;Hidetoshi Ueno .[J].Journal of Japanese Inst,1990,40:305.
[7] 张松,张春华,刘常升,文効忠.铝合金表面激光熔覆NiCrBSi的空泡腐蚀性能[J].稀有金属材料与工程,2002(02):99-102.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%