采用熔滴直接凸点制作方法,对共晶SnPb及SnAgCu钎料熔滴与Au/Ni/Cu焊盘所形成的凸点/焊盘界面组织进行了研究,并与激光重熔条件下获得的凸点/焊盘界面组织进行了比较,考察了凸点/焊盘界面组织在随后的再重熔过程中的演变.结果表明:钎料熔滴与焊盘在接触过程中形成了Au-Sn化合物,Au层并未完全反应.在随后的再重熔过程中,Au层被完全消耗,全部溶入钎料基体中,Ni层与钎料发生反应.无铅钎料(SnAgCu)和SnPb钎料所形成的界面组织明显不同;再重熔后SnPb钎料/焊盘的界面组织为Ni3Sn1,SnAgCu钎料/焊盘界面组织为(CuxNi1-x)6Sn5.
参考文献
[1] | Joachim kloeser;Paradiso Coskina;Rolf Aschenbrenner .Bump formation for flip chip and CSP by solder paste printing[J].Microelectronics and reliability,2002(3):391-398. |
[2] | Koshoubu N;Ishizawa S;Tsunetsugu H et al.Advanced flip chip bonding techniques using transferred micro-solder bumps[J].IEEE Transactions on Components Packaging and Manufacturing Technology,2000,23(02):399-404. |
[3] | Li Li;Pat Thompson .Stencil Printing Process Development for Flip Chip Interconnect[J].IEEE Transactions on Electronics Packaging Manufacturing,2000(3):165-170. |
[4] | 李福泉,王春青,田德文,田艳红,P.LIU.SnPb钎料熔滴与Au/Ni/Cu焊盘的反应过程[J].中国有色金属学报,2004(07):1139-1143. |
[5] | Qingbin Liu;Melissa Orme .High precision solder droplet printing technology and the state-of-the-art[J].Journal of Materials Processing Technology,2001(3):271-283. |
[6] | Hayes D J;Cox W R;Grove M E et al.Micro-jet printing of polymers and solder for electronics manufacturing[J].Journal of Electronics Manufacturing,1998,8(3-4):209-216. |
[7] | 王春青;李福泉 .激光直接钎料凸点制作方法[P].CN03111157,2003-09-03. |
[8] | Economikos L .Laser system for fine pitch tape automated bonding[J].Journal of Vacuum Science and Technology B:Microelectronics and Nanometer Structures,1994,12(04):2394-2399. |
[9] | James D;Hayward A.Development of laser bonding as a manufacturing process for inner lead bonding[A].San Jose, CA:SPIE,1991:164-169. |
[10] | Motullo G;Kasulke P;Heinicht K.A low cast bumping process for flip chip technology using electroless Nickel and solder ball placement[A].Tokyo:The Organizing Committee,1997:174-181. |
[11] | J. H. Lee;Y. H. Lee .FLUXLESS LASER REFLOW BUMPING OF Sn-Pb EUTECTIC SOLDER[J].Scripta materialia,2000(8):789-793. |
[12] | 田艳红,王春青.激光与红外重熔对63Sn37Pb/焊盘界面微观组织的影响[J].中国有色金属学报,2002(03):471-475. |
[13] | Bradley E.;Banerji K. .Effect of PCB finish on the reliability and wettability of ballgrid array packages[J].IEEE transactions on components, packaging, and manufacturing technology.Part B.Advanced packaging,1996(2):320-330. |
[14] | Puttlitz K.J. .Preparation, structure, and fracture modes of Pb-Sn and Pb-In terminated flip-chips attached to gold capped microsockets[J].IEEE transactions on components, hybrids, and manufacturing technology,1990(4):647-655. |
[15] | Tu KN.;Zeng K. .Tin-lead (SnPb) solder reaction in flip chip technology [Review][J].Materials Science & Engineering, R. Reports: A Review Journal,2001(1):1-58. |
[16] | 周尧和;胡壮麒;介万奇.凝固技术[M].北京:机械工业出版社,1998:75-83. |
[17] | J.Y. Park;C.W. Yang;J.S. Ha .Investigation of Interfacial Reaction Between Sn-Ag Eutectic Solder and Au/Ni/Cu/Ti Thin Film Metallization[J].Journal of Electronic Materials,2001(9):1165-1170. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%