高级检索

采用两步法合成的SiO2微球.发现氨水作为催化剂使用量过少时,SiO2微球的表面会不光滑,甚至微球的形状不规则.SiO2微球的大小主要由TEOS的初始用量和二次用量之比决定,给出了SiO2质量百分比和体积比的测量方法.

参考文献

[1] Anselmann R .[J].Journal of Nanoparticle Research,2001,3:3292336.
[2] 徐喻琼,游敏,瞿金平,郑小玲.二氧化硅增强增韧不饱和聚酯[J].华南理工大学学报(自然科学版),2008(07):106-110,116.
[3] Stober W;Fink A;Bohn E .[J].Journal of Colloid and Interface Science,1968,26:62269.
[4] Giesche H .[J].Journal of the European Ceramic Society,1994,14(03):189.
[5] Giesche H .[J].Journal of the European Ceramic Society,1994,14(03):205.
[6] Glotzer S .[J].Journal of Materials Chemistry,2003,13(10):2577.
[7] Bogush G H;Zukoski I V C F .[J].Journal of Colloid and Interface Science,1991,142:19234.
[8] Blaaderen A V;Geest J V;Vrij A .[J].Journal of Colloid and Interface Science,1992,154:4812501.
[9] Li, J;Zhao, XW;Zhao, YJ;Gu, ZZ .Quantum-dot-coated encoded silica colloidal crystals beads for multiplex coding[J].Chemical communications,2009(17):2329-2331.
[10] Zhou Z;Zhao X S .[J].Langmuir,2005,21:4717-4723.
上一张 下一张