有机高分子材料是一类重要的文物保护材料,但由于自身稳定性的限制,在紫外线照射下常发生光老化现象.因此,利用光稳定剂对其进行改性,对高性能文物保护材料的研制具有重要意义.综述了有机高分子文物保护材料的光老化机理和紫外线吸收剂、受阻胺、纳米光屏蔽剂3类常用稳定荆的稳定机理,并阐述了其在文物保护材料改性中的应用.
参考文献
[1] | 吴茂英.聚合物光老化、光稳定机理与光稳定剂(上)[J].高分子通报,2006(04):76-83. |
[2] | Forsthuber, B;Grull, G .The effects of HALS in the prevention of photo-degradation of acrylic clear topcoats and wooden surfaces[J].Polymer Degradation and Stability,2010(5):746-755. |
[3] | Fechine GJM.;Rabello MS.;Souto-Maior RM. .The effect of ultraviolet stabilizers on the photodegradation of poly(ethylene terephthalate)[J].Polymer Degradation and Stability,2002(1):153-159. |
[4] | J. Posplsil;S. Nespurek .Photostabilization of coatings. Mechanisms and performance[J].Progress in Polymer Science,2000(9):1261-1335. |
[5] | 刘景军,李效玉.高分子材料的环境行为与老化机理研究进展[J].高分子通报,2005(03):62-69. |
[6] | Ru Yu Wu et al.Pitch as a UV stabilizer for polymers[J].Polymer Degradation and Stability,1995,47(03):435. |
[7] | 黄万千;李强林;杨东洁.有机紫外线吸收剂的研究进展[J].印染,2011(20):47. |
[8] | 龚德才,何伟俊,张金萍,王鸣军.无地仗层彩绘保护技术研究[J].文物保护与考古科学,2004(01):29-32. |
[9] | 杨璐,王丽琴,黄建华,唐丽琼.改性MDI型聚氨酯文物保护材料耐光性能研究[J].文物保护与考古科学,2010(01):32-36. |
[10] | 张雪莲;唐静娟;郭时清 .丝绸的老化及保护剂的筛选[J].文物保护与考古科学,1993,5(01):17. |
[11] | Dearth MA.;Gerlock JL.;Korniski TJ. .THE LC/MS/MS CHARACTERIZATION OF PHOTOLYSIS PRODUCTS OF BENZOTRIAZOLE-BASED ULTRAVIOLET ABSORBERS[J].Polymer Degradation and Stability,1995(1):111-120. |
[12] | McGarry P;Heitner C;Schmidt J et al.A dramatic solvent effect on high-yield pulp yellowing inhibition for a benzophenone-hased ultraviolet absorber[J].Journal of Photochemistry and Photobiology A: Chemistry,2002,151(01):145. |
[13] | 杨璐,王丽琴,冯楠,黄建华,王璞,唐丽琼.文物保护用环氧树脂的光稳定剂研究[J].文物保护与考古科学,2007(04):28-32. |
[14] | 赵静,王丽琴,周文晖.唐墓彩绘文物的保护研究[J].文物保护与考古科学,2008(02):38-45. |
[15] | 邓义 .受阻胺类光稳定剂的设计、合成及表征[D].天津大学,2008. |
[16] | Gryn'ova, G.;Ingold, K.U.;Coote, M.L. .New insights into the mechanism of amine/nitroxide cycling during the hindered amine light stabilizer inhibited oxidative degradation of polymers[J].Journal of the American Chemical Society,2012(31):12979-12988. |
[17] | Yasukazu Ohkatsu .Search for Unified Action Mechanism of Hindered Amine Light Stabilizers[J].Journal of the Japan Petroleum Institute,2008(4):191-204. |
[18] | Martínez C G;Jockush S;Ruzzi M et al.Chemically induced dynamic electron polarization generated though the interaction between singlet molecular oxygen and nitroxide radicals[J].Journal of Physical Chemistry A,2005,109(45):10216. |
[19] | 王丽琴,吴晨,李迎.受阻胺类光稳定剂改性文物保护材料B72[J].精细化工,2011(06):620-624. |
[20] | 吴晨,王丽琴,李迎.受阻胺H-622改性B72及光稳定机理研究[J].文物保护与考古科学,2012(02):56-60. |
[21] | Allen NS.;Edge M.;Ortega A.;Liauw CM.;Stratton J.;McIntyre RB. .Behaviour of nanoparticle (ultrafine) titanium dioxide pigments and stabilisers on the photooxidative stability of water based acrylic and isocyanate based acrylic coatings[J].Polymer Degradation and Stability,2002(3):467-478. |
[22] | 朱世东,周根树,蔡锐,韩燕,田伟.纳米材料国内外研究进展Ⅰ--纳米材料的结构、特异效应与性能[J].热处理技术与装备,2010(03):1-5,26. |
[23] | 王敏,屠恒贤.纺织文物保护与纳米材料[J].科学(上海),2005(04):11-13. |
[24] | 李迎;王丽琴 .纳米材料在文物保护中应用的进展研究[J].材料导报,2011,25(专辑18):34. |
[25] | Petr Kotlík;Katerina Doubravová;Jírí Horálek et al.Acrylic copolymer coatings for protection against UV rays[J].Journal of Cultural Heritage,2013,15(01):44. |
[26] | Gijsman P;Smelt HJ;Schumann D .Hindered amine light stabilizers: An alternative for radiation cross-linked UHMwPE implants.[J].Biomaterials,2010(26):6685-6691. |
[27] | Caba K de la;Guerrero P .Weathering behavior of woodfaced construction materials[J].Construction and Building Materials,2007,21(06):1288. |
[28] | Custodio JEP;Eusebio MI .Waterborne acrylic varnishes durability on wood surfaces for exterior exposure[J].Progress in Organic Coatings: An International Review Journal,2006(1):59-67. |
[29] | 刘付胜聪,肖汉宁,李玉平,胡智荣,刘华斌.纳米TiO2和紫外线吸收剂对丙烯酸酯涂层抗光氧化性能的影响[J].功能材料,2004(04):495-497,500. |
[30] | Avar L.;Bechtold K. .Studies on the interaction of photoreactive light stabilizers and UV-absorbers[J].Progress in Organic Coatings: An International Review Journal,1999(1/4):11-17. |
[31] | 田丰涛,黄德音,张青.苯并三唑类紫外线吸收剂的研究进展[J].中国塑料,2000(12):12-16. |
[32] | Pandey, JK;Reddy, KR;Kumar, AP;Singh, RP .An overview on the degradability of polymer nanocomposites[J].Polymer Degradation and Stability,2005(2):234-250. |
[33] | S.M. Mirabedini;M. Sabzi;J. Zohuriaan-Mehr;M. Atai, M. Behzadnasab .Weathering performance of the polyurethane nanocomposite coatings containing silane treated TiO_2 nanoparticles[J].Applied Surface Science: A Journal Devoted to the Properties of Interfaces in Relation to the Synthesis and Behaviour of Materials,2011(9):4196-4203. |