采用熔体发泡法制备了球形孔泡沫铝及其舍金,对它们进行了拉伸试验,研究了孔隙率对拉伸性能的影响.结果表明:球形孔泡沫铝及其合金的拉伸应力-应变曲线相似,均呈现线弹性变形、平台、塑性上升、破坏四个阶段;它们的抗拉强度远低于它们的抗压强度;随孔隙率的增大它们的抗拉强度逐渐减小.
Al and Al alloy foam with spherical pores were prepared by foaming in melt, and tensile experiment was carried out to study the effect of porosity on the tensile properties. The results show that the tensile stress-strain curves of spherical pore Al foam were similar to that of spherical pore Al alloy foam. They all showed four stages of linear elastic deformation, platform, plastic increase and failure. Compared with the compressive properties of spherical pore Al and Al alloy foam, the tensile strength was far less than the compressive strength.The tensile strength decreased with the increasing porosity.
参考文献
[1] | 邹毅,何德坪,蒋家桥.新型球形孔低孔隙率高强度泡沫铝合金[J].中国科学B辑,2004(02):168-176. |
[2] | 尚金堂,何德坪.铝合金熔体中球形泡沫的生长[J].中国科学B辑,2005(03):212-219. |
[3] | K.Y.G. McCULLOUGH;N.A. FLECK;M.F. ASHBY .UNIAXIAL STRESS-STRAIN BEHAVIOUR OF ALUMINIUM ALLOY FOAMS[J].Acta materialia,1999(8):2323-2330. |
[4] | 王展光,尚金堂,何思渊,何德坪,单建.球形孔泡沫铝合金压缩性能与理论模型[J].材料热处理学报,2006(06):129-133. |
[5] | 王展光,褚旭明,何德坪,单建.强度、吸能与韧性兼容的新型球形孔泡沫纯铝[J].东南大学学报(自然科学版),2007(06):985-989. |
[6] | 王展光,徐玉红,何德坪.球形孔泡沫纯铝准静态压缩性能[J].兵器材料科学与工程,2008(04):15-19. |