The work functions before and after crystallization of two glassy alloys,Pd_(83.5)Si_(16.5) and Cu_(70)Ti_(30) have been measured by means of the con- tact potential difference method in the secondary electron field at room temperature under 10~(-5) Pa vacuum.The results show that the work functions of both glassy alloys are higher than those of the corresponding crystalline alloys.