采用脉冲激光焊接技术实现了0.5 mm厚度Hastelloy C-276屏蔽套材料对焊连接,得到的焊缝宽度小于1 mm,分析了焊接接头的拉伸性能,同时采用微区XRD分析了拉伸断口Hastelloy C-276相变特征.结果表明:焊接接头的屈服极限相对于母材并未改变;而抗拉强度有一定程度的降低,为母材的88.6%,在断口处并未发现明显脆性相.焊接接头的屈服极限与母材基本相当,主要由于焊缝处的晶粒细化效果提高了材料的屈服极限,起到了与母材固溶强化作用相似的作用;而焊接接头抗拉强度的降低主要是由于拉伸过程更利于产生应力集中,促进微观裂纹的形成,进而加速材料的破坏.

参考文献

[1] Matzie R A .[J].Nuclear Engineering and Design,2008,238:1856.
[2] 马广义,吴东江,王占宏,郭玉泉,郭东明.脉冲激光焊接对超薄Hastelloy C-276焊缝成形的影响[J].中国激光,2011(06):161-165.
[3] Cieslak M J;Headley T J;Romig A D .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1986,17A:2035.
[4] Cieslak M J;Knorovsky G A;Headley T J et al.[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1986,17A:2107.
[5] Ogborn J S;Olson D L;Cieslak M J .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,1995,203:134.
[6] Hmadm A;Khterji A;Khtarm A et al.[J].Journal of Alloys and Compounds,2005,390:88.
[7] 蒋文春,巩建鸣,陈虎,涂善东.哈氏合金C276管道焊接残余应力与变形的有限元分析[J].化工机械,2006(02):99-102,113.
[8] 唐元生,郑顺贤.PTA工程中哈氏合金(Hastelloy-C-276)管道的焊接[J].安装,2008(03):31-32.
[9] 包国平.HastelloyC276合金的焊接[J].大型铸锻件,2008(04):33-35.
[10] 毛雪平,王岗,张立殷,徐鸿,陆道钢.镍基合金C276高温拉伸力学性能的试验分析[J].动力工程,2009(07):699-702.
[11] 李婷,马雁,陆道纲.C276合金高温拉伸强度的显微分析[J].原子能科学技术,2010(06):725-729.
[12] 温鹏,获崎贤二,山本元道.环形结构激光焊接凝固热裂纹的实验研究和数值模拟[J].金属学报,2011(10):1241-1245.
[13] 杨静,程东海,黄继华,张华,赵兴科,郭和平.TC4钛合金激光焊接接头组织与性能[J].稀有金属材料与工程,2009(02):259-262.
[14] Ma G Y;Wu D J;Guo D M .[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,2011,42A:3853.
[15] Wu D J;Ma G Y;Guo Y Q et al.[J].Physics Procedia,2010,5:99.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%