采用座滴法研究了CuO对Ag/SnO2间润湿角的影响,利用扫描电镜(SEM)和电子探针显微分析(EPMA)测试了试样界面微观形貌及过渡区成分变化.结果表明,随着CuO含量的增加,SnO2与Ag的润湿性提高,7%CuO的加入,使Ag/SnO2的润湿角从90°减小到29°.加入CuO后,液态银渗入氧化物颗粒间隙,同时发生氧化物向银区的扩散,形成牢固的润湿界面.

参考文献

[1] Shen Y S;Zdanuk E J;Krock R H .The Effect of Additives from Groups IA and ⅡA on the Morphology and Properties of Silver-Cadmium Oxide Contacts[J].IEEE Transactions on PHP,1972,8(01):16-25.
[2] Wingert P C;Kim H J .Development of the Arc-Induced Erosion Surface in Silver-Cadmium Oxide[J].IEEE Transactions on Components Hybrids and Manufacturing Technology,1985,8(01):119-122.
[3] Behrens V.;Honig T. .An advanced silver/tin oxide contact material[J].IEEE Transactions on Components, Packaging, and Manufacturing Technology. Part A,1994(1):24-31.
[4] 刘海英,王亚平,丁秉钧.纳米AgSnO2触头材料的制备与组织分析[J].稀有金属材料与工程,2002(02):122-124.
[5] 王宝珠;王景琴;吕玉申 et al.Influence of Bi2O3. Additive on the Microstructure of AgSnO2 Contact Materials[J].电工合金,2000,3:7-10.
[6] Gengenbach B;Mayer U;Michal R et al.Investigation on the Switching Behavior of AgSnO2 Materials in Commercial Contactors[J].IEEE Transactions on Components Hybrids and Manufacturing Technology,1985,8(01):58-63.
[7] Jeannot D.;Pinard J. .Physical and chemical properties of metal oxide additions to Ag-SnO/sub 2/ contact materials and predictions of electrical performance[J].IEEE Transactions on Components, Packaging, and Manufacturing Technology. Part A,1994(1):17-23.
[8] 沃丁柱.复合材料大全[M].北京:化学工业出版社,2000:235-237.
[9] Ambier J.;Bourda C. .Modification in the microstructure of materials with air-break switching at high currents[J].IEEE transactions on components, hybrids, and manufacturing technology,1991(1):153-161.
[10] 黄培云.粉末冶金原理[M].北京:冶金工业出版社,1997:307-320.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%