在制备羟基磷灰石(HA)陶瓷的初期引入少量LiCl,其乙酸浸蚀失重实验表明,掺杂后HA陶瓷的耐酸蚀能力增强,HA颗粒仍然能保持较强的连接,掺杂后HA陶瓷的显微硬度稳定并有所提高,X射线衍射分析说明引入少量LiCl没有导致HA的分解.

参考文献

[1] Joschek S.;Krotz R.;Gopferich A.;Nies B. .Chemical and physicochemical characterization of porous hydroxyapatite ceramics made of natural bone[J].Biomaterials,2000(16):1645-1658.
[2] Rice RW. .GRAIN SIZE AND POROSITY DEPENDENCE OF CERAMIC FRACTURE ENERGY AND TOUGHNESS AT 22-DEGREES-C [Review][J].Journal of Materials Science,1996(8):1969-1983.
[3] Rodryguez-Lorenzo L M;Ferreira J M F .Development of porous ceramic bodies for applications in tissue engineering and drug delivery systems[J].Materials Research Bulletin,2004,39:83.
[4] 李承元,李勤,朱景和.世界锂资源的开发应用现状及展望[J].国外金属矿选矿,2001(08):22-26.
[5] 林大泽.锂的用途及其资源开发[J].中国安全科学学报,2004(09):72-76,94.
[6] Liang L. F.;Weng J.;Feng B. .Improving the Interconnectivity of Chitin-Gel-Cast Porous Calcium Phosphate Ceramics by Different Acid Etching Approaches[J].Materials Science Forum,2005(Pt.3):2367-2369.
[7] Andre M Striegel .Theory and applications of DMAc/LiCl in the analysis of polysaccharides[J].Carbohydrate Polymers,1997,34:267.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%