研究了含碳量约3.0×10-5的50W 700型号冷轧无取向硅钢板织构与磁时效的关系.200℃、24h的时效实验表明,渗碳体的时效析出阻碍磁畴壁的移动,导致试样铁损升高.磁化时180°磁畴畴壁的驱动力与硅钢板织构有密切关系,〈100〉平行于外磁场方向的织构有利于减小磁时效导致的铁损增幅,降低钢板的磁时效效应.

参考文献

[1] Ray S K;Mishra S;Mohanty O N .[J].Scripta Metallurgica,1981,15(09):971-973.
[2] 何忠治.电工钢[M].北京:冶金工业出版社,1997
[3] Nakayama T;Honjou N .[J].Journal of Magnetism and Magnetic Materials,2000,213(1-2):87-94.
[4] Khalafalla D;Morish A H .[J].Journal of Applied Physics,1972,2:624-630.
[5] Michal G M;Slane J A .[J].Jouranl of Metals,1986,38(01):32-36.
[6] Ray S K;Monanty O N .[J].Journal of Magnetism and Magnetic Materials,1989,78(04):255-262.
[7] Marraa K M;Landgrafb F J G;Buono V T .[J].Journal of Magnetism and Magnetic Materials,2008,320(20):631-634.
[8] 毛卫民;张新明.晶体材料织构定量分析[M].北京:冶金工业出版社,1995
[9] Hou C K .[J].IEEE Transzctions on Magnetics,1996,32(02):471-477.
[10] Chipman J .[J].Metallurgical and Materials Transactions,1972,3(01):55-64.
[11] 钟文定.铁磁学[M].北京:科学出版社,1992
[12] 宛德福;罗世华.磁性物理[M].北京:电子工业出版社,1987
[13] 朱宏喜,毛卫民,冯惠平.织构对CVD自支撑金刚石薄膜残余应变的影响[J].材料研究学报,2007(01):32-36.
[14] Leslie W C;Fisher R M;Sen N .[J].Acta Metallurgica,1959,7(09):632-644.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%