高级检索

设计了手机外壳冲压模具,研究了镁合金薄板温度、模具温度、拉深速度以及润滑条件对AZ31镁合金手机外壳成形质量的影响。结果表明:镁合金薄板在加热到350-400℃,且凹模的温度不低于薄板温度,较低的凸模温度(50-90℃),较低拉深速度(6mm·s^-1)及仅对薄板与凹模和压边圈接触部位润滑的条件下,可以制备出尺寸精度较高的镁合金手机外壳。

The stamping die for mobile photo shell was designed, and the effect of magnesium alloy thin sheet temperature, die temperature, drawing speed and lubricating condition on the formability quality of AZ31 magnesium alloy mobile photo shell was studied. The results show that the magnesium alloy mobile photo shell with high dimensional accuracy could be prepared successfully when the magnesium alloy thin sheet was heated to 350 -- 400 ℃, the temperature of the die was not less than that of the thin sheet, the punching speed was 6 mm · s^-1 and the position between thin sheet and blank holder, die and blank holder were lubricated.

参考文献

[1] K. Mori;H. Tsuji .Cold Deep Drawing of Commercial Magnesium Alloy Sheets[J].CIRP Annals,2007(1):285-288.
[2] 尹德良,张凯锋,吴德忠.AZ31镁合金非等温拉深性能的研究[J].材料科学与工艺,2004(01):87-90,94.
[3] 张坤,王忠堂,张士宏,于传富,许沂,王强.镁合金AZ31B板材热拉深成形工艺研究[J].轻合金加工技术,2003(10):14-17.
[4] Agnew SR;Duygulu O .Plastic anisotropy and the role of non-basal slip in magnesium alloy AZ31B[J].International Journal of Plasticity,2005(6):1161-1193.
[5] 陈振华,李展鹏,夏伟军,程永奇,严红革.热拉深工艺对镁合金制品成形性能的影响[J].机械工程材料,2006(11):13-14,94.
[6] 朱浩,周清.变形条件对AZ31镁合金塑性的影响[J].机械工程材料,2009(12):39-42.