以柠檬酸和碱式碳酸镍为原料,采用溶胶-凝胶法制备柠檬酸镍前驱体纤维,在Ar气气氛下热分解得到金属镍纤维。通过FE-SEM/EDS、DSC-TG、XRD、FT-IR和XPS对金属镍纤维的形貌、前驱体的热分解过程及纤维的物相组成进行表征。结果表明柠檬酸镍前驱体纤维在300℃热处理时出现金属Ni,且热分解过程中没有氧化镍出现。故金属镍纤维是由前驱体直接热分解形成,不经过氧化镍热还原过程。
The nickel citrate precursor fibers were prepared,using citric acid and basic nickel carbonate as the raw materials by the sol-gel method.The nickel fibers were derived from thermal decomposition of the precursors in argon gas atmosphere.The morphologies,thermal decomposition process and structure of the nickel fibers were characterized by FE-SEM/EDS,DSC-TG,XRD,FT-IR and XPS,respectively.The experimental results indicated that the nickel appeared when the heat treatment temperature was 300℃,and there was no nickel oxide existed during the whole process of the thermal decomposition.So the nickel fibers could be formed directly by the thermal decomposition of the precursor fibers,without the process of nickel oxide reduction.
参考文献
[1] | 李享成,龚荣洲.铁镍纤维的磁场诱导制备及电磁性能研究[J].功能材料,2006(01):27-28,32. |
[2] | 庾莉萍.金属纤维的特性及其开发应用[J].金属制品,2009(03):45-49. |
[3] | Hui Wu;Rui Zhang;Xinxin Liu .Electrospinning of Fe, Co, and Ni Nanofibers: Synthesis, Assembly,and Magnetic Properties[J].Chemistry of Materials: A Publication of the American Chemistry Society,2007(14):3506-3511. |
[4] | 邓橙,宋永才.溶胶-凝胶法制备镍纤维及其电磁性能研究[J].材料工程,2006(11):40-44. |
[5] | SHEN Xiang-qian;CAO Kai;ZHOU Jian-xin .Preparation of ferromagnetic binary alloy fine fibers by organic gel-thermal reduction process[J].Transactions of Nonferrous Metals Society of China,2006(5):1003-1008. |
[6] | Arranz A.;Palacio C. .Interaction of Ni/Al interfaces with oxygen[J].Langmuir: The ACS Journal of Surfaces and Colloids,2002(5):1695-1701. |
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%