用NH4F/H2O2对Br2-MeOH抛光CdZnTe晶片表面进行了表面钝化处理,通过I-V测试及XPS分析分别对钝化前后的CZT晶片的电学性能和表面组成进行了表征.I-V测试结果表明NH4F/H2O2对CdZnTe晶片表面有较好的钝化效果,电流下降率随所加偏压的增加而下降.在10V偏压下,电流下降最明显,下降率为73.7%.与欧姆定律发生偏离的临界场强为333V/cm.XPS分析发现,用NH4F/H2O2处理可使CdZnTe表面富集的Te 79.28%被氧化成TeO2,氧化层的厚度约为3.15nm.钝化后的表面更接近CdZnTe的化学计量配比.
参考文献
[1] | Chattopadhyay C;Hayes M;Ndap J O et al.[J].Journal of Electronic Materials,2000,29(06):708. |
[2] | Rybka A V;Leonov S A;Prokhoretz I M et al.[J].Nuclear Instruments and Methods in Physics Research A:Accelerators,Spectrometers,Detectors and Associated Equipment,2001,458:248. |
[3] | Chen KT.;Chen H.;Granderson B.;George MA.;Collins WE.;Burger A.;James RB.;Shi DT. .STUDY OF OXIDIZED CADMIUM ZINC TELLURIDE SURFACES[J].Journal of Vacuum Science & Technology, A. Vacuum, Surfaces, and Films,1997(3 Pt.1):850-853. |
[4] | Wright G W;Chinn D A;Brunnett D A et al.[J].SPIE,1999,3768:481. |
[5] | Wright G W;James R B;Chinn D et al.[J].Proceedings of SPIE,2000,414:324. |
[6] | Wright G W;Camarda G;Kakuno E et al.[J].Proceedings of SPIE,2004,5198:306. |
[7] | 王印月.半导体物理学[M].兰州:兰州大学出版社,1990:131. |
[8] | 陈寿椿;唐春元;于肇德.重要无机化学反应[M].上海:上海科学技术出版社,1994:947. |
[9] | 马世昌.基础化学反应[M].西安:陕西科学技术出版社,2003:280. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%