利用傅里叶变换红外光谱(FTIR)、极化曲线、交流阻抗、接触角测试和原子力显微镜(AFM)研究了全氟癸基三乙氧基硅烷(PFDS)自组装膜的结构、自组装溶液中含水量对组装膜吸附行为及缓蚀性能的影响.结果表明:通过浸泡法可以在430不锈钢表面形成PFDS自组装膜,吸附PFDS分子后,430不锈钢表面由亲水性变为疏水性;自组装溶液中含水量对膜的耐蚀性有较大的影响,且自组装膜的缓蚀效率随着自组装溶液中含水量的增大,先增大后减小.当水的体积分数为40%时,组装膜的缓蚀效率达到最大值89%.
参考文献
[1] | 余存烨.不锈钢设备及零部件酸洗钝化技术[J].清洗世界,2004(01):20-24. |
[2] | 李立清,姜平国.钢铁常温磷化工艺研究[J].腐蚀与防护,2005(07):305-306,309. |
[3] | Takeshi Kikuchi;Kunitsugu Aramaki .The inhibition effects of anion and cation inhibitors on corrosion of iron in an anhydrous acetonitrile solution of FeCl{sub}3[J].Corrosion Science,2000(5):817-829. |
[4] | Kunitsugu Aramaki;Tadashi Shimura .An Ultrathin Polymer Coating of Carboxylate Self-Assembled Monolayer Absorbed on Passived Iron to Prevent Iron Corrosion in 0.1 M Na2SO4[J].Corrosion Science,2010,52(05):1. |
[5] | 陈泽民,路品,邢海燕.铝材表面的自组装成膜新工艺[J].材料保护,2011(01):58-59,66. |
[6] | 郭增昌,王云芳,王汝敏.铝合金表面自组装膜层的表征及耐蚀性研究[J].材料保护,2007(07):1-4. |
[7] | Sinapi F;Forget L;Delhalle J et al.Self-Assembly of (3-Mercaptopropyl) Trimethoxysilane on Polycrystalline Zinc Substrates Towards Corrosion Protection[J].THIN SOLID FILMS,2002,405(112):186. |
[8] | Mekhalif Z;Sinapia F;Delhallea J .XPS and Electrochemical Evaluation of Two-Dimensional Organic Films Obtained by Chemicalmodification of Self-Assembled Monolayers of (3-Mercaptopropyl) Trimethoxysilane on Copper Surfaces[J].Material Science and Engineering,2002,22C(09):345. |
[9] | Franquet A;Lepen C;Terryn H et al.Effect of Both Concentration and Curing Time on the Structure of Non-Functional Thin Organosilane Layers on Aluminium[J].Electrochimica Acta,2003,48(09):1245. |
[10] | W.J.van Ooij;D.Zhu .Electrochemical Impedance Spectroscopy of Bis-(Triethoxysilypropyl)Tetrasulfide on Al 2024-T3 Substrates[J].Corrosion: The Journal of Science and Engineering,2001(5):413-427. |
[11] | Beccarta A M;Chtaruttini L .The Inhibitive Action of Metacryloxpropylmethoxysilane on Aluminium Corrosion in NaCl Solutions[J].Corrosion Science,1999,41(05):885. |
[12] | Zucchi F;Grassi V;Frignani A;Monticelli C;Trabanelli G .Influence of a silane treatment in the corrosion resistance of a WE43 magnesium alloy[J].Surface & Coatings Technology,2006(12/13):4136-4143. |
[13] | Montemor M F;Ptnto R;Ferreira M G S .Chemical Composition and Corrosion Protection of Silane Films Modified With CeO2 Nanoparticles[J].Electrochimica Acta,2009,54(22):5179. |
[14] | Kong, G.;Lu, J.;Zhang, S.;Che, C.;Wu, H. .A comparative study of molybdate/silane composite films on galvanized steel with different treatment processes[J].Surface & Coatings Technology,2010(2):545-550. |
[15] | Reis F M;Mwlo H G;Costa I .EIS Investigation on Al 5052 Alloy Surface Preparation for Self-Assembling Monolayer[J].Electrochimica Acta,2006,51(05):1780. |
[16] | Blajiev OL;Ithurbide A;Hubin A;Van Haesendonck C;Terryn H .XPS study of the assembling morphology of 3-hydroxy-3-phosphono-butiric acid tert-butyl ester on variously pretreated Al surfaces[J].Progress in Organic Coatings: An International Review Journal,2008(3):272-281. |
[17] | Bram C;Jung C;Stratmann M .Self Assembled Molecular Monolayers on Oxidized Inhomogeneous Aluminum Surfaces[J].Fresenius Journal of Analytical Chemistry,1997,358(1-2):108. |
[18] | Foster TT;Alexander MR;Leggett GJ;McAlpine E .Friction force microscopy of alkylphosphonic acid and carboxylic acids adsorbed on the native oxide of aluminum[J].Langmuir: The ACS Journal of Surfaces and Colloids,2006(22):9254-9259. |
[19] | Giza M;Thissen P;Grundmeier G .Adsorption kinetics of organ-ophosphonic acids on plasma-modified oxide-covered aluminum surfaces[J].Langmuir: The ACS Journal of Surfaces and Colloids,2008(16):8688-8694. |
[20] | McGovern M E;Kallury K M R;Thompson M .Role of Solvent on the Silanization of Glass With Octadecyltrichlorosilane[J].LANGMUIR,1994(10):3607. |
[21] | Gauthier S;Aime J P;Bouhacina T et al.Study of Grafted Silane Molecules on Silica Surface With an Atomic Force Microscope[J].LANGMUIR,1996,12(21):5126. |
[22] | Interaction of 12-aminododecanoic acid with a carbon steel surface: Towards the development of 'green' corrosion inhibitors[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,2010(6):p.2104. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%