低温燃料电池具有清洁、高效、可移动、操作条件温和等诸多优点.其产业化目标的实现,在很大程度上依赖于材料的改进.双极板材料性能的提高,对于延长燃料电池使用寿命和降低成本起着至关重要的作用.本文分类总结了低温燃料电池双极板材料的研发现状,比较了各种双极板材料的性能特点,并探讨了其应用前景.
参考文献
[1] | 衣宝廉.燃料电池--原理@技术@应用[M].北京:化学工业出版社,2003:45-46. |
[2] | Pellegri A;Spaziante P M .[P].US 4197178,1980-04-08. |
[3] | Lawrance R J .[P].US 4214969,1980-07-29. |
[4] | Balko E N;Lawrance R J .[P].US 4339322,1982-07-13. |
[5] | Heinzel A;Mahlendorf F;Niemzig O et al.[J].Journal of Power Sources,2004,131:35-40. |
[6] | Wilson M S;Busick D N .[P].US 6248467,2001-06-19. |
[7] | Del Rio C.;Ojeda MC.;Acosta JL.;Escudero MJ.;Hontanon E.;Daza L. .New polymer bipolar plates for polymer electrolyte membrane fuel cells: Synthesis and characterization[J].Journal of Applied Polymer Science,2002(13):2817-2822. |
[8] | Mighri F;Huneault M A;Champagne M F .[J].Polymer Engineering and Science,2004,44:1755-1765. |
[9] | Wu M;Shaw L L .[J].Journal of Power Sources,2004,136:37-44. |
[10] | Wu M;Shaw L L .[J].International Journal of Hydrogen Energy,2005,30:373-380. |
[11] | Iqbal Z;Narasinham D;Rehg T et al.[P].WO 0189013,2001-05-10. |
[12] | Bisaria M K;Andrin P;Abdou M et al.[P].US 6379795,2002-04-30. |
[13] | Saito K;Hagiwara A;Tanno F .[P].US 6242124,2001-06-05. |
[14] | Laconti A B;Griffith A E;Cropley C C et al.[P].US 6083641,2000-07-04. |
[15] | Uemura T;Murakam S .[P].US 4737421,1988-04-12. |
[16] | Emanuelson R C;Luoma W L;Taylor W A .[P].US 4301222,1981-11-17. |
[17] | Stewart R C .[P].US 4670300,1987-06-02. |
[18] | T.M.Besmann;J.W.Klett .Carbon/Carbon Composite Bipolar Plate for Proton Exchange Membrane Fuel Cells[J].Journal of the Electrochemical Society,2000(11):4083-4086. |
[19] | Woodman A S;Anderson E B;Jayne K D.[A].American Electroplaters and Surface Finishers Society,1999 |
[20] | Cisar A J;Murphy O J;Jeng K T et al.[P].US 6203936,2001-03-20. |
[21] | Brady M P;Weisbrod K;Zawodzinski C et al.[J].Electrochemical and Solid-State Letters,2002,5(11):A245-A247. |
[22] | Brady M P;Schneibel J H;Pint B A et al.[P].US 0190515,2003-10-09. |
[23] | Wang H;Brady M P;Teeter G et al.[J].Journal of Power Sources,2004,138:86-93. |
[24] | Brady M P;Weisbrod K;Paulauskas I et al.[J].Scripta Materialia,2004,50:1017-1022. |
[25] | Cho E A;Jeon U S;Hong S A et al.[J].Journal of Power Sources,2005,142:177-183. |
[26] | Li M;Luo S;Zeng C et al.[J].Corrosion Science,2004,46:1369-1380. |
[27] | Lee S J;Huang C H;Chen Y P .[J].Journal of Materials Processing Technology,2003,140:688-693. |
[28] | Iqbal Z;James T R;Guiheen V et al.[P].WO 0128019,2001-04-19. |
[29] | Mukohyama A;Takeda T;Uchida M et al.[P].WO 9750138,1997-12-31. |
[30] | Mukohyama A;Takeda T;Uchida M et al.[P].WO 9750139,1997-12-31. |
[31] | Mukohyama A;Takeda T .[P].US 5798188,1998-08-25. |
[32] | Davis J H .[P].US 0001743,2002-01-03. |
[33] | N. Cunningham;D. Guay;J. P. Dodelet .New Materials and Procedures to Protect Metallic PEM Fuel Cell Bipolar Plates[J].Journal of the Electrochemical Society,2002(7):A905-A911. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%