用15%H_2/85%Ar还原金属复合氧化物制备了 CuRh,γ-Ni_(0.33)Fe_(0.66)和α-Fe_(0.66) Co_(0.33)的合金微粉.由复合氧化物还原的TGA曲线得出还原法制备合金的温度下限.从X射线粉末衍射图的半峰宽可估算出三种微粉的粒度均小于35nm.

The ultrafine alloy powders, CuRh, γ-Ni_(0.33)Fe_(0.66) and α-Fe_(0.66)Co_(0.33) of size less than 35 nm were prepared by reduction of complex metallic oxides under atmosphere of 15%H_2 and 85% Ar.