综述了表面纳米化技术的原理和发展历程,介绍了表面纳米化技术对金属材料的疲劳性能和耐蚀性的影响,阐述和总结了在该领域中各研究者的观点.认为表面纳米层中晶粒细化及残余应力对材料性能的影响起到重要作用,超声冲击表面纳米化技术会在医用植入材料领域得到良好应用.

参考文献

[1] Lu K,Lv J.Surface Nanocrystallization (SNC) of metallic materials-presentati on of the concept behind a new Approach[J].Mater.Sci.Technol.,1999,15(3):193
[2] Tian J W,Dai K,Villegas J C.Tensile properties of a nickel-base alloy subjected to surface severe plastic deformation[J].Mater.Sci.Eng.,2008,A493(1/2):176
[3] Prakash N A,Gnanamoorthy R,Kamaraj M.Friction and wear behavior of surface nanocrystallized aluminium alloy under dry sliding condition[J].Mater.Sci.Eng.,2010,B168:176
[4] Villegas J C,Shaw L L.Nanocrystallization process and mechanism in a nickel alloy subjected to surface severe plastic deformation[J].Acta Mater.,2009,57(19):5782
[5] Shaw L,Jia W T,Angel L.A direct comparison in the fatigue resistance enhanced by surface severe plastic deformation and shot peening in a C-2000 superalloy[J].Mater.Sci.Eng.,2010,A527(4/5):986
[6] Hao Y W,Deng B,Zhong C.Effect of surface mechanical attrition treatment on corrosion behavior of 316 stainless steel[J].J.Iron Steel Res.Int.,2009,16(2):68
[7] Chen C,Li D Y,Shang C J.Nanocrystallization of aluminized surface of carbon steel for enhanced resistances to corrosion and corrosive wear[J].Electrochin.Acta,2009,55(1):118
[8] Mai Y J,Jie X H,Liu L L.Thermal stability of nanocrystalline layers fabricated by surface nanocrystallization[J].Appl.Surf.Sci.,2010,256(7):1972
[9] Dai K,Shaw L.Analysis of fatigue resistance improvements via surface severe plastic deformation[J].Int.J.Fatigue,2008,30(8):1398
[10] 王东坡,霍立兴,张玉凤.提高焊接接头疲劳强度的超声冲击法[J].焊接学报,1999,20(3):158
[11] Mordyuk B N.Fatigue life improvement of α-titanium by novel ultrasonic alloy assisted technique[J].Mater.Sci.Eng.,2006,A437:396
[12] 熊天英.0Crl 8Ni9Ti钢焊接接头表面纳米化及接头抗H2S应力腐蚀性能的研究[J].材料保护,2005,38(1):13
[13] 王吉孝.16MnR钢焊接接头表面纳米化及接头抗H2S应力腐蚀性能[J].焊接,2005,(2):13
[14] 石继红,武保林,刘刚表面纳米化对316L不锈钢抗点蚀性能的影响[J].材料保护,2008,41(5):26
[15] 王天生.1Crl 8Ni9Ti不锈钢的喷丸表面纳米化及其对耐蚀性的影响[J].机械工程学报,2005,41(9):51
[16] 吕爱强.表面纳米化对316L不锈钢性能的影响[J].材料研究学报,2005,19(2):118
[17] Barbucci A,Fame G,Matteazzi P,et al.Corrosion behaviour of nanocrystalline Cu90Ni10 alloy in neutral solution containing chlorides[J].Corros.Sci.,1999,3:463
[18] Gregory J K,Wagner L.Proceedings of the international conference on shot peening[A].ICSP8[C],2002:349
[19] Kiese J,ZhangJ,Schauerte O.Proceedings of the International Conference on Shot Peening[A].ICSP8,2002:399
[20] Wagner L,Lutjering G.Influence of Shot Peening on Fatigue Behavior of Ti Alloys in Shot Peening[M].Pergamon Press,1982
[21] Mordyuk B N.Fatigue life improvement of α-titanium by novel ultrasonic alloy assisted technique[J].Mater.Sci.Eng.,2006,A437:396
[22] Mordyuk B N,Prokopenko G I.Ultrasonic impact peening for the surface properties management[J].J.Sound.Vibration,2007,308(3-5):855
[23] 王东坡,霍立兴,张玉凤.提高焊接接头疲劳强度的超声冲击法[J].焊接学报,1999,20(3):158
[24] Hanlon T,Tabachnikova E D,Suresh S.Fatigue behavior of nanocrystalline metals and alloys[J].Int.J.Fatigue,2005,27:1147
[25] Nikitin I,Scholtes B,Maier H J.High temperature fatigue behavior and residual stress stability of laser shock peened and deep rolled austenitic steel AISI304[J].Scr.Mater.,2004,50:1345
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%