主要研究了添加Cr置换Nd5Fe72.3Cu0.2Co4B18.5合金中的Co元素对Fe3B/Nd2Fe14B型纳米复合永磁体磁性能与微观结构的影响.结果表明:相应于Co元素而言,添加Cr元素可有效细化NdFeB合金软、硬磁性相的晶粒尺寸;随退火温度的升高,添加Cr元素的Nd5Fe72.3Cu0.2Cr4B18.5合金的jHc值随退火温度的变化不明显.DTA曲线分析表明,NdFeCuCoB具有一个放热峰,而NdFeCuCrB具有两个放热峰.NdFeCuCrB非晶合金在650℃退火处理30min可获得最佳磁性能:Br=0.944T,jHc=383kA/m,(BH)max=77.5kJ/m3.
参考文献
[1] | Coehoom R;Mooij D B de;Waard C de .[J].Journal of Magnetism and Magnetic Materials,1989,80:101-104. |
[2] | Skomski R;Coey J M D .[J].Physical Review B,1993,48:15812-15816. |
[3] | Hirosawa S;Kanekiyo H;Uehara M .[J].Journal of Applied Physics,1993,73:6488-6490. |
[4] | Ping D.H.;Hono K.;Kanekiyo H.;Hirosawa S. .Mechanism of grain size refinement of Fe_3B/Nd_2Fe_14B nanocomposite permanent magnet by Cu addition[J].Journal of Applied Physics,1999(4):2448-0. |
[5] | Yoshizawa Y;Yamauchi K .[J].Materials Transactions,1990,31:3314. |
[6] | Hirosawa S;Miyoshi T;Kanekiyo H et al.[J].IEEE Transactions on Magnetics,2001,37(04):2558-2660. |
[7] | 黄胜涛.固体x射线学[M].北京:高等教育出版社,1985:314. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%