利用渣-钢热力学平衡研究了CaO-MgO-SiO2-Al2O3-FetO-MnO-P2O5渣系对钢水二次氧化的行为.得到了渣中FetO活度的近似表达式.在固定FetO摩尔分数的条件下,FetO的活度系数在炉渣碱度(NCaO+NMgO+NMnO)/(NSiO2+NAl2O3+NP2O5)达到2.5左右时出现最大值;而MnO的活度系数则随碱度的增加逐渐增大.γFetO(L)在NFetO固定时,随渣中(CaO)/(SiO2)的增大而减小;γMnO(L)随NMnO增加而减小.