采用粉末冶金法制备了具有适合人体组织长入孔径的多孔钛,并对其进行生物活化处理.利用EPMA、SEM、XRD等研究了不同预处理方法和浸泡时间对多孔钛表面羟基磷灰石(HA)的形貌及形成速度的影响.结果表明,多孔钛的表面以及孔的内表面上均有纳米晶TiO2生成,预钙化处理能够明显提高多孔钛表面生成羟基磷灰石的速率,促进HA的形核长大,预钙化后磷含量增加明显,验证了Na2HPO4在预处理中对多孔钛的活化是有利的.
参考文献
[1] | Hench LL .Biomaterials: a forecast for the future.[J].Biomaterials,1998(16):1419-1423. |
[2] | Vehof JWM.;Jansen JA.;Spauwen PHM. .Bone formation in calcium-phosphate-coated titanium mesh[J].Biomaterials,2000(19):2003-2009. |
[3] | Ferretti C;Ripamonti U .Human segmental mandibular defects treated with naturally derived bone morphogenetic proteins.[J].The Journal of craniofacial surgery,2002(3):434-444. |
[4] | Sun L M;Berndt C C;Gross K A et al.Material fundamentals and clinical performance of plasma-sprayed hydroxyapatite coatings:a review[J].Journal of Biomedical Materials Research,2001,58(05):570-592. |
[5] | Witt J D;Swann M .Metal wear and tissue response in failed titanium alloy total hip replacements[J].Journal of Bone and Joint Surgery-British Volume,1991,73B(04):559-563. |
[6] | Thieme M;Wieters K P;Bergner F et al.Titanium powder sintering for preparation of a porous functionally graded material destined for orthopaedic implants[J].Journal of Materials Science,2001,12:225-231. |
[7] | Kokubo T;Takadama H .How useful is SBF in predicting in vivo bone bioactivity?[J].Biomaterials,2006(15):2907-2915. |
[8] | 梁芳慧,王克光,周廉.预钙化处理后的钛表面磷灰石涂层的形成[J].材料科学与工程,2002(04):541-544,533. |
[9] | Wen HB.;Dewijn JR.;Liu Q.;Cui FZ.;Degroot K.;Wolke JGC. .FAST PRECIPITATION OF CALCIUM PHOSPHATE LAYERS ON TITANIUM INDUCED BY SIMPLE CHEMICAL TREATMENTS[J].Biomaterials,1997(22):1471-1478. |
[10] | Kokubo T;Kim H M;Kawashita M et al.Bioactivemetals:preparation and properties[J].Journal of Materials Science,2004,15(01):99-107. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%