采用四点弯曲的试验研究方法,对爆炸焊接不锈钢-铝复层材料界面断裂性能进行了研究,采用扫描电子显微镜对界面裂纹与断口形貌进行观察分析.研究结果表明:采用爆炸焊接工艺可以达到不锈钢-铝复层板的良好结合,以界面能量释放率作为界面断裂韧性的评价指标,其平均值为1.725 Mpa·m.界面断口可以观察到清晰的爆炸焊接波纹痕迹,并且有微观裂纹的存在,界面断裂整体倾向于脆性断裂.
参考文献
[1] | Joho W Hutchinson.Advances in Applied Mechanics[M].USA:Academic Press,1992:112. |
[2] | Jiang F et al.[J].International Journal of Pressure Vessels and Piping,2003,80:129. |
[3] | Serier B et al.[J].COMPUTATIONAL MATERIALS SCIENCE,2004,29:309. |
[4] | Odowd N P et al.[J].Philosophical Magazine A:Physics of Condensed Matter:Structure Defects and Mechanical Properties,1992,66(06):1037. |
[5] | Qing Ma .[J].Journal of Materials Research,1997,12:840. |
[6] | 蔡昊 et al.[J].上海力学,1997,18:241. |
[7] | Tschegg E et al.[J].Acta Metallurgica Et Materialia,1990,38:469. |
[8] | Lucksanasombool P.;Higgs WAJ.;Higgs RJED.;Swain MV. .Interfacial fracture toughness between bovine cortical bone and cements[J].Biomaterials,2003(7):1159-1166. |
[9] | Klingbeil N W et al.[J].Engineering Fracture Mechanics,1997,56:113. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%